Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 4000 µm | <= 4000 µm | Grain Size |
Gouda Vuurvast CURON 110 Dense Refractory Castable Description: Curon 110 is an easily workable castable, especially developed to cast complicated shapes. Because of its low shrinkage, this castable has less tendency to crack.Remarks: These values a.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | Grain Size |
Gouda Vuurvast CURON 140 Dense Refractory Castable Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this castable can be applied up to 1400°C in slightly reducing atmospheres. Up to high temperatures Curo.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | Grain Size |
Gouda Vuurvast CURON 140 GM Dense Refractory Castable Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this gunning castable can be applied up to 1400°C in slightly reducing atmospheres.Remarks: These values.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | Grain Size |
Gouda Vuurvast FLUCON 150 Dense Self Flowing Refractory Castable Description: Flucon 150 is a self-flowing low cement castable based on sintered bauxite.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | Grain Size |
Gouda Vuurvast FLUCON 160 H SiC (R) Dense Self Flowing Refractory Castable Description: Flucon 160 H SiC (R) is a self-flowing low cement castable, characterized by a high strength and good slag resistance. Because of the presence of SiC this material has a very good resis.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | Grain Size |
Gouda Vuurvast GOLITE 125 GM Refractory Insulating Castable Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast... |
|||
Particle Size | <= 4000 µm | <= 4000 µm | Grain Size |
Gouda Vuurvast VIBRON 150 G RAPID Dense Vibrating Refractory Castable Description: Vibron 150 G Rapid is a low cement castable based on sintered South-American bauxite. Because of special additives this material is suited for direct contact with liquid aluminum and al.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | Grain Size |
Gouda Vuurvast CURON 127 S GM Dense Refractory Castable Description: Curon 127 S GM gunning castable is characterized by a reasonable strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks:.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | Grain Size |
Gouda Vuurvast CURON 145 Dense Refractory Castable Description: Because of the use of pure raw materials, Curon 145 has a low Fe2O3 content. Therefore this castable is widely used in reducing atmospheres.Remarks: These values apply to cast products... |
|||
Particle Size | <= 4000 µm | <= 4000 µm | Grain Size |
Gouda Vuurvast CURON 150 GM Dense Refractory Castable Description: Curon 150 GM is a gunmix based on sintered bauxite with an excellent thermal shock resistance and is therefore very well suited for burner blocks.Remarks: These values apply to cast pro.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | Grain Size |
Gouda Vuurvast GOLITE 95 Refractory Insulating Castable Description: Golite 95 is widely applied as an insulating backlining behind a dense castable, especially in the petrochemical industry.Remarks: These values apply to cast products. Also available in.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | Grain Size |
Gouda Vuurvast VIBRON 155 Dense Vibrating Refractory Castable Description: Vibron 155 is a vibrating castable based on sintered bauxite especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provid.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9035 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9230 D 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9230 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9255 0.09 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9335 MG 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9335 MG 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9335 MG 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9435 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9435 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9230 A 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9230 A 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9230 D 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9235 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9235 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9235 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9255 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9255 0.08 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |
|||
Particle Size | <= 4000 µm | <= 4000 µm | |
BASF Neopolen® P 9435 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |