Material Notes:
Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to measure the physical properties, parts with dimensions 300x200x60 mm were molded on a machine typical for the EPP industry under standard conditions. The properties can vary depending on part geometry and processing parameters.Information provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.0260 - 0.0300 g/cc
0.000939 - 0.00108 lb/in³
Density 0.0500 g/cc
0.00181 lb/in³
ISO 845
Water Absorption <= 1.0 %

@Time 86400 sec
<= 1.0 %

@Time 24.0 hour
DIN 53428
Particle Size >= 2500 µm
>= 2500 µm
<= 4000 µm
<= 4000 µm
Mechanical Properties Metric English Comments
Tensile Strength 0.740 MPa
107 psi
DIN EN ISO 1798
Elongation at Break 30 %
30 %
DIN EN ISO 1798
Compressive Strength 0.240 MPa

@Strain 10.0 %
34.8 psi

@Strain 10.0 %
ISO 844
0.290 MPa

@Strain 25.0 %
42.1 psi

@Strain 25.0 %
ISO 844
0.440 MPa

@Strain 50.0 %
63.8 psi

@Strain 50.0 %
ISO 844
Compression Set 27 %

@Temperature 23.0 °C,
Time 79200 sec
27 %

@Temperature 73.4 °F,
Time 22.0 hour
50% RH; 24h after stress release; DIN EN ISO 1856 (Procedure C)
Thermal Properties Metric English Comments
Thermal Conductivity 0.0370 W/m-K
0.257 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 120 - 180 °C
248 - 356 °F
Decomposition Temperature >= 180 °C
>= 356 °F
Flash Point >= 200 °C
>= 392 °F
ASTM D1929
Electrical Properties Metric English Comments
Surface Resistance <= 1.00e+12 ohm
<= 1.00e+12 ohm
DIN IEC 60093
Descriptive Properties Value Comments
Average Particle Weight 0.6 - 1.0 mg
Color Black
Commercial Status Europe
Dimensional Stability at Heat <2%
Linear size alterations after 4 d, 110°C; DIN ISO 2796
Ignition Temperature > 360 °C
ASTM D1929