Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 1.0 µm | >= 1.0 µm | 10% smaller than |
Nyco 10 AS WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | >= 1.0 µm | >= 1.0 µm | 10% smaller than |
Nyco 10 WOLLASTOCOAT® Wollastonite Chemically treated grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Particle Size | >= 1.0 µm | >= 1.0 µm | 10% smaller than |
Nyco NYAD® 5000 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Particle Size | >= 1.0 µm | >= 1.0 µm | 10% smaller than |
Nyco NYAD® M1250 Wollastonite Fine particle size grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Particle Size | 1.0 - 2.0 µm | 1.0 - 2.0 µm | |
Nabaltec NABALOX® NO 615-30 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 1.0 µm | 1.0 µm | |
Poco Graphite ZXF-5Q Industrial Grade Graphite SSH hardness is 86.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small p.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 63% of particles less than |
Old Hickory No. 1 Glaze Kentucky Ball Clay No. 1 Glaze Clay is a very high kaolin bearing selection with extremely low levels of carbon content. it provides excellent suspension to all types of glazes especially glazes containing a high perc.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 60% of particles less than |
Old Hickory No. 5 Kentucky Ball Clay No. 5 clay is a kaolinitic ball clay containing low levels of carbon. It provides high suspension and plasticity to a variety of ceramic formulations and is an excellent source of Al2O3 content. No... |
|||
Particle Size | 1.0 µm | 1.0 µm | 61% of particles less than |
Old Hickory No. 6 Kentucky Ball Clay No. 6DC is a highly kaolin clay that can be used as a filler grade material where presence of some 200 M quartz residue is not harmful. Applications can include a variety of refractory compositions .. |
|||
Particle Size | 1.0 µm | 1.0 µm | 62% of particles less than |
Old Hickory Volunteer Tennessee Ball Clay A versatile clay selection for casting, pressing, or plastic forming process methods. It is similar to M-23 in mineralogy with slightly more organic content. Volunteer has very good plasticity and i.. |
|||
Particle Size | <= 1.0 µm | <= 1.0 µm | |
Poco Graphite EDM-AF5 EDM Graphite POCO's EDM-AF5 is the only graphite electrode material available on the market today with an average particle size of less than one micron. This particle structure gives EDM-AF5 superior strength, p.. |
|||
Particle Size | 1.0 µm | 1.0 µm | Median Grain Diameter |
Nabaltec APYRAL® 60D Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 47% finer than |
Imerys Allenâ„¢ G Kaolin Allen G is an intermediate-grained kaolin used as a suspension aid in ceramic glazes.Information provided by Imerys |
|||
Particle Size | 1.0 µm | 1.0 µm | 86% finer than |
Imerys Amlockâ„¢ 321 Kaolin Information provided by Imerys |
|||
Particle Size | 1.0 µm | 1.0 µm | 86% finer than |
Imerys Barnetâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 1.0 µm | 1.0 µm | 46.5% finer than |
Imerys Franklin™ R Kaolin Franklin R is an intermediate-grained Kaolin used as a filler is “soft†rubber products, plastic compounds, adhesives, protective coatings and similar applications.Information provided by .. |
|||
Particle Size | 1.0 - 2.0 µm | 1.0 - 2.0 µm | FSSS |
H.C. Starck Ampersint® MAP FeCoNi 70/10/20 For Hardmetals High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a .. |
|||
Particle Size | 1.0 - 2.0 µm | 1.0 - 2.0 µm | FSSS |
H.C. Starck Ampersint® MAP FeNi 50/50 For Hardmetals High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a .. |
|||
Particle Size | 1.0 - 3.0 µm | 1.0 - 3.0 µm | Laser Diffraction D50 |
H.C. Starck Standard 120 Titanium Carbide, TiC Hard metals (tooling and machining)CementsBlack ceramics, e.g. (Al2O3-TiC) |
|||
Particle Size | <= 1.0 µm | <= 1.0 µm | 5% |
SGL Carbon Group CF 270 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | <= 1.0 µm | <= 1.0 µm | 2% |
SGL Carbon Group CF 3100 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | 1.0 µm | 1.0 µm | D10 (Malvern) Size E |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | <= 1.0 µm | <= 1.0 µm | Grain Size |
CoorsTek Superstrate® 996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Particle Size | 1.0 µm | 1.0 µm | Median |
Excalibar ExBar™ W 1 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Particle Size | 1.0 µm | 1.0 µm | Median |
CIMBAR CIMBAR™ EX Barite Powder (BaSO4) CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical .. |
|||
Particle Size | 1.0 µm | 1.0 µm | Median |
CIMBAR Miti-Wite B1 Chemically Purified White Barite (BaSO4) Miti-Wite barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. Miti-Wite products are available in a variety of particle sizes .. |
|||
Particle Size | 1.0 µm | 1.0 µm | @ 10% |
CIMBAR RP 9410 Talc RP 9400 Series talcs are produced from ores, which provide an excellent balance of mechanical properties at an economical price, for primary use in commodity polypropylene. RP 9400 Series talcs are.. |
|||
Particle Size | >= 1.0 µm | >= 1.0 µm | 10% smaller than |
Nyco 10 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |