Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.400 µm | 0.400 µm | Average Stokes Equivalent Diameter |
KaMin KaMin® 611 Kaolin Clay - Waterwashed Naturally delaminated clay for use in water-based paints and coatings.Industry: Paint & CoatingsUses: Industrial Coatings, E-Coat, PrimerInformation provided by KaMin LLC. |
|||
Particle Size | 0.400 µm | 0.400 µm | Average Stokes Equivalent Diameter |
KaMin KaMin® 90 Kaolin clay - Waterwashed KaMin® 90 is a high brightness, fine particle size, general-purpose filler with moderate water demand. KaMin® 90 is ideally suited for solvent and water-borne paint, ink and adhesive applicati.. |
|||
Particle Size | 0.400 µm | 0.400 µm | Average Stokes Equivalent Diameter |
KaMin KaMin® 90B Kaolin Clay - Waterwashed KaMin® 90B is a high brightness, fine particle size, general-purpose filler with moderate water demand. KaMin® 90B is ideally suited for water-borne applications where high gloss, holdout and .. |
|||
Particle Size | 0.400 µm | 0.400 µm | Median (Malvern Laser) |
KaMin KaMin® HG90 Kaolin Clay - Ultrafine, high brightness KaMin® HG90 is a high brightness, ultra-fine particle size, platy kaolin with moderate water demand providing good tinting strength, Ti02 extension and gloss in water based paints. KaMin® HG90.. |
|||
Particle Size | 0.400 µm | 0.400 µm | Average Stokes Equivalent Diameter |
KaMin Lithosperse® 7005CS Kaolin Clay - Surface Treated Lithosperse® 7005 CS is a high performance treated kaolin designed to improve rheology with outstanding dispersibility and resistance to clay bleed in lithographic cold set inks. Lithosperse® .. |
|||
Particle Size | 0.400 µm | 0.400 µm | Median (Malvern Laser) |
KaMin Nucap® 190W Kaolin Clay - Surface Treated Reinforcing filler/extender for elastomeric systems. Nucap®190W is a high brightness treated kaolin used in white roofing membranes and white sidewalls. Silane treated clays mix in quicker and ma.. |
|||
Particle Size | 0.400 µm | 0.400 µm | Median (Malvern Laser) |
KaMin Nucap® 290W Kaolin Clay - Surface Treated Reinforcing filler/extender for elastomeric systems. Nucap®290W is a high brightness kaolin with the highest level of surface treatment to impart the best mechanical properties and water resistan.. |
|||
Particle Size | 0.400 µm | 0.400 µm | Median (Malvern Laser) |
KaMin Nulok® 390 Kaolin Clay - Surface Treated High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R.. |
|||
Particle Size | 0.400 µm | 0.400 µm | Median (Malvern Laser) |
KaMin Polygloss® 90 Kaolin Clay - Ultrafine, high brightness Ultrafine, highly pulverized, premium brightness kaolin for extending high gloss solvent and water-based coatings.Industry: Paint & Coatings, Rubber & Plastic, InkUses: Architectural Coatings, Indus.. |
|||
Particle Size | 0.400 µm | 0.400 µm | Average Stokes Equivalent Diameter |
KaMin Polyfil® F Kaolin Clay - Waterwashed Water washed kaolin clays such as Polyfil® F offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® F is a moderate brightness water .. |
|||
Particle Size | 0.400 µm | 0.400 µm | Average Stokes Equivalent Diameter |
KaMin Polyfil® FB Kaolin Clay - Waterwashed Water washed kaolin clays such as Polyfil® FB offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® FB is a moderate brightness wate.. |
|||
Particle Size | 0.400 µm | 0.400 µm | Median (Malvern Laser) |
KaMin Polyfil® HG90 Kaolin Clay - Waterwashed High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R.. |