KaMin Nucap® 290W Kaolin Clay - Surface Treated

Category Ceramic , Clay , Kaolin Clay
Manufacturer KaMin LLC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KaMin Nucap® 290W Kaolin Clay - Surface Treated.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Reinforcing filler/extender for elastomeric systems. Nucap®290W is a high brightness kaolin with the highest level of surface treatment to impart the best mechanical properties and water resistance. Silane treated clays mix in quicker and may allow the formulator to reduce the amount of added silane. The treatment aids dispersion in soft, low shear compounds such as stoppers, tubing, and printing blankets.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl Rubber, EPDMInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Brightness 91 %
91 %
Reflectance (TAPPI)
Moisture Absorption at Equilibrium <= 1 %
<= 1 %
As Produced
Particle Size 0.200 µm
0.200 µm
Average Stokes Equivalent Diameter
0.400 µm
0.400 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.005% Retained
pH 6
6
100 g/250 ml H2O Slurry
Specific Surface Area 22.0 m²/g
22.0 m²/g
BET
Descriptive Properties Value Comments
CAS Number Proprietary
Crystalline Silica (quartz) <0.1%
Physical Form Dry
Shipping Point Wrens, GA