Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

KaMin Polyfil® F Kaolin Clay - Waterwashed

Category Ceramic , Clay , Kaolin Clay
Manufacturer KaMin LLC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KaMin Polyfil® F Kaolin Clay - Waterwashed.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Water washed kaolin clays such as Polyfil® F offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® F is a moderate brightness water washed kaolin. It has a higher brightness and offers improved consistency compared to air-floated clays. Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, Polyolefins/PVC, SMC/BMC, EPDM, Mold ReleaseInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Bulk Density 0.192 - 0.240 g/cc
0.00694 - 0.00868 lb/in³
Loose
Brightness 88 %
88 %
Reflectance (TAPPI)
Oil Absorption 43 %
43 %
Fineness >= 5
>= 5
Hegman Grind
Moisture Absorption at Equilibrium <= 1.5 %
<= 1.5 %
As Produced
Particle Size 0.400 µm
0.400 µm
Average Stokes Equivalent Diameter
1.50 µm
1.50 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.005% Retained
pH 7
7
100 g/250 ml H2O Slurry
Specific Surface Area 17.0 m²/g
17.0 m²/g
BET
Descriptive Properties Value Comments
Bulking Value 21.7 lb.gal
CAS Number 1332-58-7
Crystalline Silica (quartz) <0.1%
Physical Form Dry
Shipping Point Macon, GA