Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.900 - 1.10 g/cc | 0.0325 - 0.0397 lb/in³ | |
Nabaltec NABALOX® NO 103 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D4745 |
3M Dyneon™ CC146/S Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of 60% bronze blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Bulk Density | <= 0.900 g/cc | <= 0.0325 lb/in³ | |
Magyar Aluminum ALOLT 730 Aluminum Hydroxide Viscosity Optimized Type |
|||
Bulk Density | <= 0.900 g/cc | <= 0.0325 lb/in³ | |
Magyar Aluminum ALOLT 8AF Aluminum Hydroxide Ground type |
|||
Bulk Density | 0.900 - 1.10 g/cc | 0.0325 - 0.0397 lb/in³ | |
Magyar Aluminum ALO-P90 Alumina Alumina for Polishing |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 60 |
Lanxess Pocan® DP 7102 000000 PBT, 32% Mineral PBT, 32% mineral, injection molding, LDSInformation provided by LANXESS. |
|||
Bulk Density | 0.900 - 1.20 g/cc | 0.0325 - 0.0434 lb/in³ | |
Solvay Chemicals Oxyper® S131 Sodium Percarbonate Oxyper® S131 is a stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in bleach additive products and environmental applications; it may be suitabl.. |
|||
Bulk Density | 0.900 - 1.20 g/cc | 0.0325 - 0.0434 lb/in³ | |
Solvay Chemicals Oxyper® SHC Sodium Percarbonate Oxyper® SHC is a high coated, stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in bleach additive products, detergent powders and tablets, autom.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
Sharadaa Ceramics 26 Insulation Bricks-ASTM Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
Sharadaa Ceramics HFI Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFINSUL 8S Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Bulk Density | 0.900 g/cc @Temperature 200 °C |
0.0325 lb/in³ @Temperature 392 °F |
|
Sharadaa Ceramics Sharada LTM 0.9 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | Powder Density; ASTM D1895 |
Sumitomo Bakelite North America E 8398 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Vyncolit, a Sumitomo B.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America Epiall® 1904B-1 Short Glass Fiber Reinforced Epoxy Epiall 1904B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided .. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America Epiall® 1908-1 Short Glass Fiber Reinforced Epoxy Epiall 1908-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation proper-ties that meets the requir.. |
|||
Bulk Density | 0.900 - 1.30 g/cc | 0.0325 - 0.0470 lb/in³ | tapped |
Solvay Chemicals Strontium carbonate standard powder Strontium carbonate standard powder is used in the production of ferrites for permanent magnets. Strontium carbonate standard powder is also used for the production of glazes and enamel frits.Inform.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America Epiall® 1908B-1 Short Glass Fiber Reinforced Epoxy Epiall 1908B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided .. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
A. Schulman POLYBATCH™ White B8750A Concentrate Based In HDPE DescriptionPOLYBATCH® B8750A is a specialty white masterbatch based in HDPE. This product has been designed to achieve optimum dispersion and excellent letdown mixing in blow molding applications... |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | Tap |
TIMCAL TIMREX® FC250-1500 Coke TIMREX Petroleum Coke is calcined at appropriate temperature with low ash and sulfur (sulphur) content, well defined texture and consistent particle size distribution.Advantages and applications: S.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | Size D (tapped) |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
A. Schulman POLYBATCH™ White B8750A Concentrate Based In HDPE DescriptionPOLYBATCH® B8750A is a specialty white masterbatch based in HDPE. This product has been designed to achieve optimum dispersion and excellent letdown mixing in blow molding applications... |
|||
Bulk Density | >= 0.900 g/cc | >= 0.0325 lb/in³ | |
Chosun Refractories LW-30 Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
BASF Sicopal® Green K 9610 Color Additive Chemical Structure: Co/Ti/Ni/Zn-oxideApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA PETP, CA/CAB and UPRecommendations for food applicat.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
BASF Sicotan® Brown K 2611 Color Additive Chemical Structure: Mn/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
BASF Sicotan® Brown K 2711 Color Additive Chemical Structure: Mn/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
BASF Sicotan® Yellow K 1010 Color Additive Chemical Structure: Ni/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Plenco 1510 Polyester, Granular, Transfer Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America Epiall® 1908M-1 Short Glass Fiber Reinforced Epoxy Epiall 1908M-1 is a short glass fiber reinforced epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information provided.. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America Epiall® 1961B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy Epiall 1961B-1 is a short glass fiber and mineral filled epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information .. |
|||
Bulk Density | 0.900 g/cc | 0.0325 lb/in³ | |
A. Schulman POLYBATCH™ White B8750A Concentrate Based In HDPE DescriptionPOLYBATCH® B8750A is a specialty white masterbatch based in HDPE. This product has been designed to achieve optimum dispersion and excellent letdown mixing in blow molding applications... |