Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | Tapped |
Nyco NYAD® 5000 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | Poured; ASTM D1895 |
Eastman A12 PET
(discontinued **) Voridian Polymer A12 is currently produced to Eastman`s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer A12 is available i.. |
|||
Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | Poured; ASTM D1895 |
Eastman CB11E PET
(discontinued **) VORIDIAN PET CB11E is designed specifically for the carbonated soft drink (CSD) and other beverage markets in the European market area. The polymer delivers faster, more efficient processing and bet.. |
|||
Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | |
Invista 1101 PET Copolymer Packaging Resin
(discontinued **) Carboxyl end groups: |
|||
Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | |
Invista 3301 PET Copolymer Packaging Resin
(discontinued **) Carboxyl end groups: |
|||
Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | |
Invista 3302 PET Copolymer Packaging Resin
(discontinued **) Carboxyl end groups: |
|||
Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | ISO 60 |
FKuR Kunststoff Bio-Flex® F 1130 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | ASTM D1895 |
Plenco 1500 Polyester, Granular, Compression Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | ASTM D1895 |
Plenco 1581 Polyester, Pellet, Injection Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |
|||
Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | ASTM D1895 |
Plenco 7556 Phenolic, Briquette, Transfer Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |
|||
Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | |
DuPont™ Nomex® N196 Paper, 20 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | |
Daikin NEOFLON AC-5820 PFA Coating Powder, White NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Electrostatic sp.. |
|||
Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | ASTM D4894-98a |
3M Dyneon™ TFM™ 1600 PTFE Meets ASTM D4894 Type III, Grade 2 resinMolding and ram extrusion powder with very good free flowing propertiesGood metering propertiesGood mold filling behaviorImproved particle coalescenceDenser p.. |
|||
Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | ASTM D4894-98a |
3M Dyneon™ TF 1641 PTFE Meets ASTM D4894 Type IV, Grade 2 resinMolding and ram extrusion powder very good free-flow propertiesGood metering propertiesGood mold filling behaviorGood electrical and mechanical propertiesVery .. |
|||
Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | ASTM D4894-98a |
3M Dyneon™ TF 1645 PTFE Meets ASTM D4894 Type IV, Grade 2 resinMolding and ram extrusion powder very good free-flow propertiesGood metering propertiesGood mold filling behaviorGood electrical and mechanical propertiesUsed .. |
|||
Bulk Density | >= 0.830 g/cc | >= 0.0300 lb/in³ | Pycnometer test |
Invista 1101R Copolymer Packaging Resin
(discontinued **) Carboxyl end groups: |