Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® CM Galileo Europa 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® LN 5000 Expandable Polystyrene Extir LN 5000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strength, e.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® Verdi VR A3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir Verdi VR A3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not con.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® Verdi VR A5000 AE Expandable Polystyrene - Flame Retardant b>Product Description:Extir Verdi VR A5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® CM Galileo Io 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® CM Galileo Io 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® CM Giotto 5 AE Expandable Polystyrene - Continuous Mass/Flame Retardant Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain CFC.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® GEO 3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir GEO 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain C.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® LN 7000 Expandable Polystyrene Extir LN 7000 belongs to the product family, the Leonardo Series, with these features: high expandability, high moulding productivity, wide processing area, optimal fusion and mechanical strenght, e.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir Leonardo A 5000 AE Expandable Polystyrene
(discontinued **) Extir A 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir Leonardo A 7000 AE Expandable Polystyrene
(discontinued **) Extir A 7000 AE is a flame retardant expandable polystyrene in the form of spherical beads of large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 7.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir Leonardo B 2000 AE Expandable Polystyrene
(discontinued **) Extir B 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir B 200.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir Leonardo B 5000 AE Expandable Polystyrene
(discontinued **) Extir B 5000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene
(discontinued **) Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or CFC. Extir D 30.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene
(discontinued **) Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® F 1111 Expandable Polystyrene
(discontinued **) Extir F 1111 is an expandable polystyrene in the form of spherical beads of very fine particle size and a narrow particle size distribution, containing pentane as blowing agent. Extir does not cont.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® P 1212 Expandable Polystyrene
(discontinued **) Extir P 1212 is an expandable polystyrene in the form of spherical beads of very fine particle size and narrow distribution, containing pentane as blowing agent. Extir does not contain CFC or HCFC. .. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 94312 HDPE Extrusion Coating Resin
(discontinued **) Resin Type: Melt blend, FDA approvedCharacteristics: Good processabilityGood drawdown capabilityImproved MVTR propertiesGrease resistanceApplications: MVTR applicationsRelease linersCup stockInforma.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | |
SGL Carbon Group CF 270 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | |
Silon TA 2347 HD Orange Catalyst Masterbatch Masterbatch for use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD.TA 2347 HD, together with the above mentioned graft, contains the cross-linking catalyst to complete a Sioplas System... |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | |
Silon Taborex TA 2329 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 1117 HD. TA 2329 HD contains a cross-linking catalyst and a stabiliser package. Together with the above-mentioned grafted P.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | |
Silon Taborex TA 2330 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TABOREX TA 1117 HD. TA 2330 HD contains a cross-linking catalyst and a stabiliser package. Together with the above-mentioned g.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | |
Zircar Ceramics IB-100A Alumina Bubble Thin wall aluminum oxide ceramic spheres offered in 2 standard bubble sizes. These low density sintered ceramic bodies are useful in a range of refractory applications with temperatures to 2000°C (.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | Tap |
TIMCAL TIMREX® T150-600 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | Loose |
Nyco ULTRAFIBRE® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Plenco 7579 Phenolic, Granular, Injection Molded PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ISO 60 |
Vyncolit Neopreg Kinel® SK4525 S5 Glass Fiber Reinforced Molding Compound BMI molding compound long glass fiber reinforced with excellent mechanical and thermal properties. Especially suited to be used for injection molding.Information provided by Sumitomo Bak North Ameri.. |