Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | Tapped |
Nyco NYAD® M1250 Wollastonite Fine particle size grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | Tapped |
Nyco NYAD® MD1250 Wollastonite Fine particle size grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | C-186 |
I. Stern IS-7985 Polyethylene Terephthalate Resin Product Description: IS-7985 is a natural polyethylene terephthalate (PET) resin. This resin is produced by continuous melt phase polymerization followed by solid phase polymerization.Certificatio.. |
|||
Bulk Density | 0.870 - 0.970 g/cc | 0.0314 - 0.0350 lb/in³ | |
Solvay Chemicals Ixper® 25M Magnesium Peroxide IXPER® 30M Magnesium Peroxide Granules are based on our commercial grade IXPER® 35M.EINECS Number: 215-627-7/CAS Number: 1335-26-8Information provided by Solvay |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D1895 |
Plenco 1530 Polyester, Briquette, Injection Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D1895 |
Plenco 5118 Phenolic, Granular, Compression Molded PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorptio.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D1895 |
Plenco 5118 Phenolic, Granular, Transfer Molded PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorptio.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D1895 |
Plenco 7556 Phenolic, Briquette, Injection Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | Vibrated; ASTM D1895 |
Eastman Aqua PJ003 PET Voridian Aqua PET PJ003 is a condensation polymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. This product is specifically designed f.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | |
DuPont™ Nomex® 410 Paper, 5 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | DAK-QAR-SOP-0018 |
DAK Americas Laser+® B90A PET Laser+® (B90A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Bi-orientation of Laser+® (B.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | DAK-QAR-SOP-0018 |
DAK Americas Laser+® B90B PET Product Description: Laser+® (B90B) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Typical .. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | DAK-QAR-SOP-0018 |
DAK Americas Laser+® C (C60A) PET Product Description: Laser+® C (C60A) is a unique copolymer particularly suited for use in the custom PET container applications where clarity and neutral colored are desired. It is a medium intrin.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | DAK-QAR-SOP-0018 |
DAK Americas Laser+® C (E60A) PET Product Description: Laser+® C (E60A) is a unique copolymer particularly suited for use in the custom PET container applications where clarity and neutral colored are desired. It is a medium intrin.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | DAK-QAR-SOP-0018 |
DAK Americas Laser+® C C61A PET Product Description: Laser+® C (C61A) is a unique copolymer particulary suited for use in the custom PET container applications where clarity and neutral color and desired. It is a medium intrinsic.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | DAK-QAR-SOP-0018 |
DAK Americas Laser+® C E61A PET Product Description: Laser+® C (E61A) is a unique copolymer particularly suited for use in the custom PET container applications where clarity and neutral color and desired. It is a medium intrinsi.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | DAK-QAR-SOP-0018 |
DAK Americas Laser+® C K62A PET Laser+® C (K62A) is a unique copolymer particularly suited for use in both the BCF (bulk continuous filament) production of fibers and custom PET container application where clarity and neutral col.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | DAK-QAR-SOP-0018 |
DAK Americas Laser+® HS D59A PET Product Description: Laser+® HS (D59A) polyethylene terephthalate (PET) resin is designed for conversion to PET packaging by injection stretch blow-molding using commercial heat-set technology.Typi.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | DAK-QAR-SOP-0018 |
DAK Americas Laser+® W L40A PET Product Description: Laser+® W (L40A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Typica.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | DAK-QAR-SOP-0018 |
DAK Americas Laser+® W L40B PET Product Description: Laser+® W (L40B) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Typica.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | DAK-QAR-SOP-0018 |
DAK Americas Laser+® W L44A PET Product Description: Laser+® W (L44A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Typica.. |
|||
Bulk Density | 0.870 g/cc | 0.0314 lb/in³ | DAK-QAR-SOP-0018 |
DAK Americas Laser+® W L44B PET Product Description: Laser+® W (L44A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Typica.. |