Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm @Time 86400 sec |
0.0082 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP FARADEX DX11003 PC (Europe-Africa-Middle East) LNP FARADEX DX11003 is a compound based on Polycarbonate resin potentially suitable to meet high frequency electromagnetic absorption requirments. The compound is also an excellent candidate for man.. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm @Time 86400 sec |
0.0082 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU (Asia Pacific) LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm @Time 86400 sec |
0.0082 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36S PPA LNP LUBRICOMP* UFL36S is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant, Bearing Grade. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm @Time 86400 sec |
0.0082 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36S PPA (Asia Pacific) LNP LUBRICOMP* UFL36S is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm @Time 86400 sec |
0.0082 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXC PPA LNP* LUBRICOMP* UFL36SXC is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm @Time 86400 sec |
0.0082 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXC PPA (Asia Pacific) LNP* Lubricomp* UFL36SXC is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm @Time 86400 sec |
0.0082 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXP PPA LNP LUBRICOMP* UFL36SXP is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm @Time 86400 sec |
0.0082 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXQ PPA LNP* LUBRICOMP* UFL36SXQ is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15%PTFE. Added features of this material include: Wear Resistant, Heat Stabilized, Bearing Grade. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm @Time 86400 sec |
0.0082 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXQ PPA (Asia Pacific) LNP* Lubricomp* UFL36SXQ is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm @Time 86400 sec |
0.0082 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm @Time 86400 sec |
0.0082 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Asia Pacific) LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm @Time 86400 sec |
0.0082 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Europe-Africa-Middle East) LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm @Time 86400 sec |
0.0082 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-LOY PF306 PA 6 LNP* STAT-LOY* PF306 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added feature of this grade includes: Antistat. |
|||
Linear Mold Shrinkage, Transverse | 0.0082 cm/cm @Time 86400 sec |
0.0082 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas re.. |