Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0074 cm/cm @Time 86400 sec |
0.0074 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP KONDUIT MT00E PP LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing 70% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0074 cm/cm @Time 86400 sec |
0.0074 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP KONDUIT MT00E PP (Asia Pacific) LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0074 cm/cm @Time 86400 sec |
0.0074 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP KONDUIT MT00E PP (Europe-Africa-Middle East) LNP KONDUIT* MT00E is a compound based on Polypropylene resin containing Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0074 cm/cm @Time 86400 sec |
0.0074 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC LNP* LUBRICOMP* DX98306H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Linear Mold Shrinkage, Transverse | 0.0074 cm/cm @Time 86400 sec |
0.0074 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC (Asia Pacific) LNP* Lubricomp* DX98306H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Linear Mold Shrinkage, Transverse | 0.0074 cm/cm @Time 86400 sec |
0.0074 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ.. |
|||
Linear Mold Shrinkage, Transverse | 0.0074 cm/cm @Time 86400 sec |
0.0074 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 (Asia Pacific) LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia P.. |
|||
Linear Mold Shrinkage, Transverse | 0.0074 - 0.0081 cm/cm @Time 86400 sec |
0.0074 - 0.0081 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP SF006 PA 12 LNP THERMOCOMP* SF006 is a compound based on Nylon 12 resin containing 30% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0074 - 0.0081 cm/cm @Time 86400 sec |
0.0074 - 0.0081 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp SF006S PA 12 LNP* Thermocomp* SF006S is a compound based on Nylon 12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |