Coating Weight 20.2 g/m²
12.6 lb/ream
ExxonMobil Method
ExxonMobil Label-Lyte™ 33LL247 OPP Film
Product Description: A super white opaque, high gloss, caviated BOPP film designed for use in reel-fed warp-around labeling applications where superior graphics are desired.Availability: Africa & Mi..
Coating Weight 20.2 g/m²
12.6 lb/ream
ExxonMobil Method
ExxonMobil Label-Lyte™ 38DL247 OPP Film
Product Description: A super white opaque, high gloss, high yield and highly cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired.Av..
Coating Weight 20.2 g/m²
12.6 lb/ream
ExxonMobil Method
ExxonMobil Oppalyte™ 38DO447 OPP Film
Product Description: A super white opaque BOPP film. The Diamex technology allows for super low density and very high yield. Diamex makes it possible to lower the density, without decreasing the mod..
Coating Weight 20.2 g/m²
12.6 lb/ream
ExxonMobil Method
ExxonMobil Oppalyte™ 33ICE OPP Film
Product Description: Coextruded white opaque, low density, biaxially oriented polypropylene film. This film is designed for the ice cream applications, and is suitable for heat seal and cold seal on..
Coating Weight 20.2 g/m²
12.6 lb/ream
ExxonMobil Method
ExxonMobil Oppalyte™ 33MW247 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa ..