Polymer Property : Coating Weight = 23.2 g/m² Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 23.2 g/m²
14.5 lb/ream
ExxonMobil Method
ExxonMobil Label-Lyte™ 38LL247 OPP Film
Product Description: A super white opaque, high gloss, cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired.Availability: Africa & M..
Coating Weight 23.2 g/m²
14.5 lb/ream
ExxonMobil Method
ExxonMobil Label-Lyte™ 38LW280 OPP Film
Product Description: A super white opaque slip controlled, biaxially oriented polypropylene film, metalized on one side. Designed for use in reel-fed wrap-around applications, where outstanding meta..
Coating Weight 23.2 g/m²
14.5 lb/ream
ExxonMobil Method
ExxonMobil Metallyte™ 38ICE M OPP Film
Product Description: A coextruded super white opaque, low density, biaxially oriented polypropylene film, metalized on one side. This film is designed for HFFS applications, heat seal or cold seal.A..
Coating Weight 23.2 g/m²
14.5 lb/ream
ExxonMobil Method
ExxonMobil Metallyte™ 38MW280 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film, metalized on one side. Ideal for single web packaging applications on HFFS in combination with cold seal.Availability..
Coating Weight 23.2 g/m²
14.5 lb/ream
ExxonMobil Method
ExxonMobil Metallyte™ 38MW480 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film, metalized on one side.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features: Outstanding opacity an..
Coating Weight 23.2 g/m²
14.5 lb/ream
ExxonMobil Method
ExxonMobil Oppalyte™ 38ICE OPP Film
Product Description: A coextruded white opaque, low density, biaxially oriented polypropylene film. This film is designed for the ice cream applications, and is suitable for heat seal and cold seal ..
Coating Weight 23.2 g/m²
14.5 lb/ream
ExxonMobil Method
ExxonMobil Oppalyte™ 38MO447 OPP Film
Product Description: A coextruded white opaque, low density, biaxially oriented polypropylene film, heat sealable on the inside. The treated layer must be printed and varnished to provide the necess..
Coating Weight 23.2 g/m²
14.5 lb/ream
ExxonMobil Method
ExxonMobil Oppalyte™ 38MW247 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa ..