Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.60 g/cc | 0.0579 lb/in³ | |
Garlock BLUE-GARD® 3300 Compressed Aramid Fiber Gasketing, Neoprene Binder Aramid fiber, high-temperature fillers, and neoprene (CR) binder. Handles service conditions with refrigerants and various petroleum-based oils. Excellent SealabilityUnique blend of aramid fibers, f.. |
|||
Density | 1.60 g/cc | 0.0579 lb/in³ | |
Garlock BLUE-GARD® 3400 Compressed Aramid Fiber Gasketing, SBR Binder Aramid fiber, high-temperature fillers, and SBR binder. Often used in low-pressure saturated steam applications.Excellent SealabilityUnique blend of aramid fibers, fillers, and a SBR rubber binder p.. |
|||
Density | 1.60 g/cc | 0.0579 lb/in³ | |
Garlock BLUE-GARD® 3000 Compressed Aramid Fiber Gasketing, Nitrile Binder Aramid fiber, high-temperature fillers, and nitrile (NBR) binder.Excellent SealabilityUnique blend of aramid fibers, fillers, and a NBR rubber binder provides improved torque retention and lowered e.. |
|||
Density | 1.60 g/cc @Temperature 121 °C |
0.0579 lb/in³ @Temperature 250 °F |
Dry Density |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M33 Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or .. |
|||
Density | 1.60 g/cc | 0.0579 lb/in³ | Wet Density |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M44 Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or .. |
|||
Density | 1.60 - 1.76 g/cc | 0.0579 - 0.0637 lb/in³ | |
Saint-Gobain Chemfab® SlipGrip™ 3 PTFE/Silicone Coated Fiberglass Fabric Description: SlipGrip™ products are PTFE-coated fiberglass fabrics with silicone rubber on one face. This unique combination provides a "slippery" PTFE surface and a "grippy" silicone surface. .. |
|||
Density | 1.60 g/cc | 0.0579 lb/in³ | |
BNZ Materials Transite HT Low Temperature Industrial Board These non-asbestos, monolithic fiber cement industrial boards are used in environments up to 1000°F where high strength is the primary concern. These fiber cement boards are used in the foundry ind.. |
|||
Density | 1.60 g/cc | 0.0579 lb/in³ | |
Garlock BLUE-GARD® 3700 Compressed Aramid Fiber Gasketing, EPDM Binder Aramid fiber, high-temperature fillers, and EPDM binder. For service areas with weak causticsExcellent SealabilityUnique blend of aramid fibers, fillers, and a EPDM rubber binder provides improved t.. |