Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.25 - 1.72 g/cc | 0.0452 - 0.0621 lb/in³ | Average value: 1.54 g/cc Grade Count:5 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep.. |
|||
Density | 1.13 - 1.72 g/cc | 0.0408 - 0.0621 lb/in³ | Average value: 1.37 g/cc Grade Count:195 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Density | 1.58 - 1.72 g/cc | 0.0571 - 0.0621 lb/in³ | Average value: 1.69 g/cc Grade Count:14 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Density | 1.20 - 1.72 g/cc | 0.0434 - 0.0621 lb/in³ | Average value: 1.45 g/cc Grade Count:331 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Density | 1.68 - 1.72 g/cc | 0.0607 - 0.0621 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 108 Halogen Free PVC Filling and bedding, designed to meet BS 6724 |
|||
Density | 1.68 - 1.72 g/cc | 0.0607 - 0.0621 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HFC 0108 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding, designed to meet BS 6724Information provided by Fainplast Compounds |
|||
Density | 1.52 - 1.72 g/cc | 0.0549 - 0.0621 lb/in³ | Molded |
Bulk Molding Compounds BMC T60-6009 Compression Grade Wear Resistant Molding Compound BMC T60-6009 is a compression grade wear resistant molding compound. This material was specifically formulated for applications that require excellent abrasion resistance. Due to its low specific .. |