Fainplast Compounds HAX HF 108 Halogen Free PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name HAX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds HAX HF 108 Halogen Free PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Filling and bedding, designed to meet BS 6724
Physical Properties Metric English Comments
Density 1.68 - 1.72 g/cc
0.0607 - 0.0621 lb/in³
IEC 60811
Melt Index of Compound 10 g/10 min

@Load 21.6 kg,
Temperature 150 °C
10 g/10 min

@Load 47.6 lb,
Temperature 302 °F
Fainplast
Mechanical Properties Metric English Comments
Hardness, Shore D 41 - 47
41 - 47
IEC 60811
Tensile Strength at Break 6.00 MPa
870 psi
IEC 60811
Elongation at Break 100 %
100 %
IEC 60811
Thermal Properties Metric English Comments
Oxygen Index 34 %
34 %
ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm

@Temperature 20.0 °C
>= 1.00e+13 ohm-cm

@Temperature 68.0 °F
ASTM D257