Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.08 - 1.08 g/cc @Temperature 285 - 285 °C |
0.0390 - 0.0390 lb/in³ @Temperature 545 - 545 °F |
Average value: 1.08 g/cc Grade Count:2 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Density | 1.08 - 1.08 g/cc @Temperature 300 - 300 °C |
0.0390 - 0.0390 lb/in³ @Temperature 572 - 572 °F |
Average value: 1.08 g/cc Grade Count:5 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Density | 1.00 - 1.08 g/cc | 0.0361 - 0.0390 lb/in³ | Average value: 1.04 g/cc Grade Count:12 |
Overview of materials for Nylon 11, Flexible Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Flexible Tubing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Density | 1.02 - 1.08 g/cc | 0.0368 - 0.0390 lb/in³ | Average value: 1.05 g/cc Grade Count:5 |
Overview of materials for Nylon 12, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Graphite Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Density | 1.03 - 1.08 g/cc | 0.0372 - 0.0390 lb/in³ | |
Lord Adhesives 206 Long Working Time Acrylic Adhesive Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f.. |
|||
Density | 1.07 - 1.08 g/cc | 0.0387 - 0.0390 lb/in³ | |
Guarniflon TENFIL TF 200 Polytetrafluoroethylene Thread Sealant TENFIL TF200 is a PTFE-based thread sealant in water dispersion, which increases the tightness of the threaded parts and prevents leakage of water. The product is intended for the assembly of fitti.. |
|||
Density | 1.02 - 1.08 g/cc | 0.0368 - 0.0390 lb/in³ | ASTM D 792 |
Karina E 5525/1-TRE Kariprene Natural. Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Density | 1.04 - 1.08 g/cc | 0.0376 - 0.0390 lb/in³ | |
Shandong Guangyin PA 612 Nylon Resin Features and Applications: As one kind of nylon with better tenacity, PA612 is mainly applicable to coating of high-grade toothbrush monofilaments, monofilaments and cables.Information provided by S.. |
|||
Density | 0.959 - 1.08 g/cc | 0.0346 - 0.0390 lb/in³ | |
3M 1000NF Fast Tack Water Based Adhesive 3M™ Fast Tack Water Based Adhesive 1000NF is a high performance water-based, one part adhesive formulated for fast bonding and long term heat resistant bonds.Information provided by 3M |
|||
Density | 1.04 - 1.08 g/cc | 0.0376 - 0.0390 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 565A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Density | 1.01 - 1.08 g/cc | 0.0365 - 0.0390 lb/in³ | |
3M 32665 Green Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Density | 1.01 - 1.08 g/cc | 0.0365 - 0.0390 lb/in³ | |
3M 32666 Tan Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Density | 1.04 - 1.08 g/cc | 0.0376 - 0.0390 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 570A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Density | 1.01 - 1.08 g/cc | 0.0365 - 0.0390 lb/in³ | |
3M 32663 Medium Grey Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Density | 1.01 - 1.08 g/cc | 0.0365 - 0.0390 lb/in³ | |
3M 32664 Light Gray Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |