Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.60 - 7.80 g/cc | 0.275 - 0.282 lb/in³ | |
PSM Industries Pacific Sintered Metals Nickel Silver BZN-131-U Powdered Metal Higher strength than brass, Good corrosion resistance Equivalent MPIF Specification: CZN-1818-17Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 7.60 g/cc | 0.275 lb/in³ | |
PSM Industries PolyAlloys MIM-17-4 PH Heat Treated Stainless Steel Information Provided by PolyAlloys, a division of PSM Industries |
|||
Density | 7.60 g/cc | 0.275 lb/in³ | |
PSM Industries PolyAlloys MIM-2200 Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Density | 7.60 g/cc | 0.275 lb/in³ | |
Piezo Kinetics 402 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type I, it is designed to serve as a driver where high power and low losses are dictated by design. It is primarily well suited for ultrasonic cleaners and sonars.Elastic Compliance .. |
|||
Density | 7.60 g/cc | 0.275 lb/in³ | |
Piezo Kinetics 700 Lead Zirconate Titanate Piezoelectric This material has low dielectric constant, high QM, high shear coupling coefficient, good temperature stability and low aging characteristics. Common use of this material is in delay lines and accel.. |
|||
Density | 7.60 g/cc | 0.275 lb/in³ | |
Piezo Kinetics 802 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type III, it is specifically used as a driver that exhibits low losses under extreme driving conditions and has a high Q. PKI 804 is well suited for medical applications.Elastic Comp.. |
|||
Density | 7.60 - 7.80 g/cc | 0.275 - 0.282 lb/in³ | |
PSM Industries Pacific Sintered Metals Bronze BT-126 Powdered Metal Higher strength structural and bearing bronzeInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 7.60 - 7.80 g/cc | 0.275 - 0.282 lb/in³ | |
Pacific Sintered Materials BZ-111-U Yellow Brass Powdered Metal Applications: 80-20 leaded brass for structural and hardware components.Equivalent MPIF Specification: CZP-2000-11All information provided by Pacific Sintered Metals. |
|||
Density | 7.60 g/cc | 0.275 lb/in³ | Sintered |
Kinetics MIM 4605 Low Alloy Steel (As Sintered) Low alloy steel, carbon, nickel, molybdenum. A multi-purpose, economical material that offers various strength, hardness, and wear resistance properties depending if it is heat treated and the heat .. |
|||
Density | 7.60 g/cc | 0.275 lb/in³ | Sintered |
Kinetics MIM 4605 Low Alloy Steel (Case Hardened) Low alloy steel containing carbon, nickel, molybdenum. A multi-purpose, economical material that offers various strength, hardness and wear resistance properties depending if it is heat treated and .. |
|||
Density | 7.61 g/cc @Temperature 399 °C |
0.275 lb/in³ @Temperature 750 °F |
hardened to 62 HRC |
Bohler-Uddeholm AISI D2 Cold Work Tool Steel AISI D2 is a high-carbon, high-chromium tool steel alloyed with molybdenum and vanadiumAISI AD2 is characterized by: High wear resistance High compressive strength Good through-hardening properties.. |
|||
Density | 7.60 g/cc @Temperature 400 °C |
0.275 lb/in³ @Temperature 752 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
Density | 7.60 g/cc @Temperature 500 °C |
0.275 lb/in³ @Temperature 932 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
Density | 7.60 g/cc @Temperature 600 °C |
0.275 lb/in³ @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
Density | 7.62 g/cc | 0.275 lb/in³ | |
Carlson Nitronic® 60® Austenitic Stainless Steel General DescriptionNitronic 60 is an anti-galling and wear resistant austenitic stainless steel. It provides a significantly lower cost alternative to combat wear and galling when compared with cob.. |
|||
Density | 7.61 g/cc | 0.275 lb/in³ | |
AK Steel 409 Ferritic Stainless steel AK Steel 409 Stainless Steels are especially useful for applications where oxidation or corrosion protection beyond the capacity of carbon steel and some coated steels is needed. Current applicatio.. |
|||
Density | 7.60 g/cc | 0.275 lb/in³ | |
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 15% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
Density | 7.61 g/cc @Temperature 400 °C |
0.275 lb/in³ @Temperature 752 °F |
|
Assab Steels ASSAB XW-42 Cold Work Steel XW-42 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength High hardness after hardeningGood through-hardeni.. |
|||
Density | 7.61 g/cc @Temperature 400 °C |
0.275 lb/in³ @Temperature 752 °F |
|
Assab Steels ASSAB XW-5 Cold Work Steel ASSAB XW-5 is a high-carbon, high chromium tool steel alloyed with tungsten, characterized by:High wear resistanceHigh compressive strengthHigh surface hardness after hardeningGood through-hardening.. |
|||
Density | >= 7.60 g/cc | >= 0.275 lb/in³ | |
Channel Industries 5500 Lead Zirconate Titanate Piezoelectric Navy Type IICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most exten.. |
|||
Density | 7.60 g/cc | 0.275 lb/in³ | |
ArcelorMittal Save 20-13 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Density | 7.60 g/cc | 0.275 lb/in³ | |
ArcelorMittal Save 20-15 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Density | 7.60 g/cc | 0.275 lb/in³ | |
ArcelorMittal Save 25-14 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Density | 7.60 g/cc | 0.275 lb/in³ | |
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 10% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
Density | 7.60 g/cc | 0.275 lb/in³ | |
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 25% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
Density | 7.60 g/cc | 0.275 lb/in³ | |
PSM Industries PolyAlloys MIM-316L sintered Stainless Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Density | 7.60 - 7.80 g/cc | 0.275 - 0.282 lb/in³ | |
Pacific Sintered Materials BT-126 Bronze Powdered Metal Applications: Higher strength structural and bearing bronze.All information provided by Pacific Sintered Metals. |
|||
Density | 7.62 g/cc | 0.275 lb/in³ | |
HP Alloys Nitronic® 60 Austenitic Stainless, Annealed Annealed applies to tensile and/or hardness; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was originally designed as a high tempe.. |
|||
Density | 7.62 g/cc | 0.275 lb/in³ | |
HP Alloys Nitronic® 60 Austenitic Stainless, Level 4 Cold Worked Level 4 Cold Worked applies to tensile properties of 0.25 to 2 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was origin.. |