| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| PSM Industries PolyAlloys MIM-2200 sintered Low Alloy Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| PSM Industries PolyAlloys MIM-2200 Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| PSM Industries PolyAlloys MIM-2700 sintered Low Alloy Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| Piezo Kinetics 402 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type I, it is designed to serve as a driver where high power and low losses are dictated by design. It is primarily well suited for ultrasonic cleaners and sonars.Elastic Compliance .. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| Piezo Kinetics 532 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type V, this ceramic is used as sensors that require low impedance, high dielectric constant and high sensitivity.Elastic Compliance s11E (x 10-12 m²/n): 15.9.Elastic Compliance s33.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| Piezo Kinetics 552 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type VI, this ceramic is used as sensors that require extremely high dielectric constant and large displacements. PKI 556 material has been slightly modified to give a higher g33 val.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| Piezo Kinetics 700 Lead Zirconate Titanate Piezoelectric This material has low dielectric constant, high QM, high shear coupling coefficient, good temperature stability and low aging characteristics. Common use of this material is in delay lines and accel.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| Piezo Kinetics 802 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type III, it is specifically used as a driver that exhibits low losses under extreme driving conditions and has a high Q. PKI 804 is well suited for medical applications.Elastic Comp.. |
|||
| Density | 7.60 - 7.80 g/cc | 0.275 - 0.282 lb/in³ | |
| Pacific Sintered Materials BZN-131-U Nickel Silver Powdered Metal Higher strength than brass. Good corrosion resistance.Equivalent MPIF Specification: CZN-1818-17All information provided by Pacific Sintered Metals. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | Sintered |
| Kinetics MIM 4605 Low Alloy Steel (Case Hardened) Low alloy steel containing carbon, nickel, molybdenum. A multi-purpose, economical material that offers various strength, hardness and wear resistance properties depending if it is heat treated and .. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| Goodfellow Cobalt/Silicon/Boron/Manganese Alloy Information provided by Goodfellow.Composition Notes: Si + B content = 25 wt%. Fe+Mo content = 2 wt%. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| CMW® ELKALOY D Copper Alloy, Aluminum Bronze ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and th.. |
|||
| Density | 7.60 g/cc @Temperature 400 °C |
0.275 lb/in³ @Temperature 752 °F |
|
| Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| Carpenter Gall-Tough PLUS™ Stainless, Annealed Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 4.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| Carpenter Gall-Tough PLUS™ Stainless, Annealed, 15% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| ArcelorMittal Save 20-13 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| ArcelorMittal Save 20-15 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| ArcelorMittal Save 25-14 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| ArcelorMittal Save 25-16 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| ArcelorMittal Save 27-15 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| ArcelorMittal Save 27-17 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| ArcelorMittal Save 30-15 Electrical Steel Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| ArcelorMittal Speed 35-440 Electrical Steel Properties: The iCARe™ Speed product family comes with guaranted losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| ArcelorMittal Speed 35-510 Electrical Steel Properties: The iCARe™ Speed product family comes with guaranted losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| Carpenter Gall-Tough PLUS™ Stainless, Annealed, 0% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| Carpenter Gall-Tough PLUS™ Stainless, Annealed, 10% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
| Density | 7.60 g/cc | 0.275 lb/in³ | |
| PSM Industries PolyAlloys MIM-316L sintered Stainless Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
| Density | 7.60 - 7.80 g/cc | 0.275 - 0.282 lb/in³ | |
| Pacific Sintered Materials BT-126 Bronze Powdered Metal Applications: Higher strength structural and bearing bronze.All information provided by Pacific Sintered Metals. |
|||