Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.46 g/cc | 0.270 lb/in³ | |
Indium Corp. Indalloy® 8 In-Sn-Cd Fusible Alloy General purpose fusible alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.47 g/cc | 0.270 lb/in³ | |
Crucible Steel CPM® S30V® Stainless Steel CPM S30V is a martensitic stainless steel designed to offer the best combination of toughness, wear resistance and corrosion resistance. Its chemistry has been specially balanced to promote the form.. |
|||
Density | 7.47 g/cc | 0.270 lb/in³ | |
Crucible Steel CPM® S35VN™ Stainless Steel CPM S35VN is a martensitic stainless steel designed to offer improved toughness over CPM S30V. It is also easier to machine and polish than CPM S30V. Its chemistry has been rebalanced so that it for.. |
|||
Density | 7.47 g/cc | 0.270 lb/in³ | |
Crucible Steel CSM® S60V (440V) Tool Steel, AISI 440C Modified CPM S60V is a unique tool steel made by the Crucible Particle Metallurgy process. It is designed from a 440C stainless base analysis with added high carbon and vanadium for exceptionally good wear r.. |
|||
Density | 7.47 g/cc | 0.270 lb/in³ | hardness of 60 HRC |
Bohler-Uddeholm UDDEHOLM VANADIS 6 Cold Work Tool Steel Description: Chromium-molybdenum-vanadium alloyed PM steel. Toolmaking with highly alloyed tool steel means that machining and heat treatment have to be considered more than with lower alloyed grade.. |
|||
Density | 7.47 g/cc | 0.270 lb/in³ | |
AK Steel 400 Ferritic Stainless steel AK Steel 400 is one of the most economical chromium ferritic stainless steels. It has corrosion and oxidation resistance comparable to Type 410 stainless steel with good fabricating characteristics.. |
|||
Density | 7.48 g/cc | 0.270 lb/in³ | |
ATI Allegheny Ludlum Ohmaloy® 30 Resistance Alloy Ohmaloy 30 alloy is a moderately magnetic, ductile stainless steel having extremely high electrical resistivity. In addition to imparting high electrical resistivity, the aluminum content in these .. |
|||
Density | 7.48 g/cc | 0.270 lb/in³ | |
ATI Allegheny Ludlum ALFA-I™ Stainless Steel Type 406 Characteristics:superior oxidation resistance for the temperature range 1600°F-over 2200°F, high electrical resistivity, high resistance to sulfidation, high resistance to carburization. Applicat.. |