AK Steel 400 Ferritic Stainless steel

Category Metal , Ferrous Metal , Ferritic , Stainless Steel , T 400 Series Stainless Steel
Manufacturer AK Steel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AK Steel 400 Ferritic Stainless steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AK Steel 400 is one of the most economical chromium ferritic stainless steels. It has corrosion and oxidation resistance comparable to Type 410 stainless steel with good fabricating characteristics. AK Steel 400 contains no titanium, so its surface is free of titanium streaks. This provides improved appearance, and alleviates die wear that may be caused by titanium stabilized chromium steels. AK Steel 400 is non-hardenable by heat treatment because of its low carbon content which also minimizes hardening during welding. Typical applications include heat exchangers, display racks, gas range burner rings, office furniture and other uses where corrosion resistance at minimum cost is important.Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.47 g/cc
0.270 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 72
72
Tensile Strength, Ultimate 469 MPa
68000 psi
Tensile Strength, Yield 234 MPa

@Strain 0.200 %
33900 psi

@Strain 0.200 %
Elongation at Break 30 %
30 %
in 2 inches
Modulus of Elasticity 200 GPa
29000 ksi
Thermal Properties Metric English Comments
CTE, linear 10.8 µm/m-°C

@Temperature 24.0 - 260 °C
6.00 µin/in-°F

@Temperature 75.2 - 500 °F
12.8 µm/m-°C

@Temperature <=871 °C
7.11 µin/in-°F

@Temperature <=1600 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F

@Temperature 32.0 - 212 °F
Thermal Conductivity 24.9 W/m-K

@Temperature 100 °C
173 BTU-in/hr-ft²-°F

@Temperature 212 °F
28.6 W/m-K

@Temperature 500 °C
198 BTU-in/hr-ft²-°F

@Temperature 932 °F
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.25 %
<= 0.25 %
Carbon, C <= 0.050 %
<= 0.050 %
Chromium, Cr 12 - 13 %
12 - 13 %
Iron, Fe >= 84.64 %
>= 84.64 %
As Remainder
Manganese, Mn <= 1.0 %
<= 1.0 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000600 ohm-cm
0.0000600 ohm-cm