Crucible Steel CPM® S30V® Stainless Steel

Category Metal , Ferrous Metal , Martensitic , Stainless Steel
Manufacturer Crucible Steel
Trade Name CPM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel CPM® S30V® Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CPM S30V is a martensitic stainless steel designed to offer the best combination of toughness, wear resistance and corrosion resistance. Its chemistry has been specially balanced to promote the formation of vanadium carbides which are harder and more effective than chromium carbides in providing wear resistance. CPM S30V offers substantial improvement in toughness over other high hardness steels such as 440C and D2, and its corrosion resistance is equal to or better than 440C in various environments.The CPM process produces very homogeneous, high quality steel characterized by superior dimensional stability, grindability, and toughness compared to steels produced by conventional processes.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 7.47 g/cc
0.270 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 255
255
Annealed
Hardness, Rockwell C 58 - 61
58 - 61
Modulus of Elasticity 221 GPa
32100 ksi
Charpy Impact 13.56 J
10.00 ft-lb
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 20.0 - 200 °C
6.11 µin/in-°F

@Temperature 68.0 - 392 °F
Thermal Conductivity 17.31 W/m-K

@Temperature 93.0 °C
120.1 BTU-in/hr-ft²-°F

@Temperature 199 °F
Shrinkage -0.100 - -0.0500 %
-0.100 - -0.0500 %
Component Elements Properties Metric English Comments
Carbon, C 1.45 %
1.45 %
Chromium, Cr 14 %
14 %
Iron, Fe 78.55 %
78.55 %
As Remainder
Tungsten, W 2.0 %
2.0 %
Vanadium, V 4.0 %
4.0 %