Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.141 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 3.90 - 3.92 g/cc
0.141 - 0.142 lb/in³
Sintered
Nabaltec GRANALOX® NM 9922 B Ceramic Body, Binder Free
Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti..
Density 3.90 g/cc
0.141 lb/in³
Nabaltec NABALOX® NO 103 Calcined Aluminum Oxide
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.90 g/cc
0.141 lb/in³
Nabaltec NABALOX® NO 105 Calcined Aluminum Oxide
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.90 g/cc
0.141 lb/in³
Nabaltec NABALOX® NO 105 RA Calcined Aluminum Oxide
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.90 g/cc
0.141 lb/in³
Nabaltec NABALOX® NO 105-71 Calcined Aluminum Oxide
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.90 g/cc
0.141 lb/in³
Nabaltec NABALOX® NO 115-G Ground Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.90 g/cc
0.141 lb/in³
Nabaltec NABALOX® NO 313 Ground Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.90 g/cc
0.141 lb/in³
Nabaltec NABALOX® NO 615-30 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.90 g/cc
0.141 lb/in³
Nabaltec NABALOX® NO 625-10 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.89 g/cc
0.141 lb/in³
Sintered Density
Nabaltec NABALOX® NO 625-30 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.90 g/cc
0.141 lb/in³
Sintered
Nabaltec NABALOX® NO 713-10 MF Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.90 g/cc
0.141 lb/in³
Nabaltec NABALOX® NO 713-10 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.90 g/cc
0.141 lb/in³
Nabaltec NABALOX® NO 713-40 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.90 g/cc
0.141 lb/in³
Nabaltec NABALOX® NO 715-10 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.90 g/cc
0.141 lb/in³
Nabaltec NABALOX® NO 725-10 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.90 g/cc
0.141 lb/in³
NanoScale NanoActive® Aluminum Oxide
NanoActive Al2O3 is produced using proprietary processes to obtain high specific surface area, low density, amorphous material with high adsorption capacity and chemical reactivity. NanoActive Al2O3..
Density 3.90 g/cc
0.141 lb/in³
ASTM 1457-62 T
Fluorseals PTFE 60% bronze filled
Improved compressive strength and thermal conductivity.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Density 3.90 g/cc
0.141 lb/in³
Misumi Alumina 99 Aluminum Oxide, Al2O3
Information provided by MISUMI Corporation.
Density 3.89 g/cc
0.141 lb/in³
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to..
Density 3.90 g/cc
0.141 lb/in³
ASTM D792
Techmer ES HiFill® PA6 0390 BK
Availability: North AmericaForms: PelletsFeatures: High Specific GravityAppearance: BlackInformation provided by TP Composites, Inc.
Density 3.90 g/cc
0.141 lb/in³
Sapco 98% Aluminum Oxide
Information provided by Sapco.
Density 3.90 g/cc
0.141 lb/in³
DIN EN 623-2 / ASTM-C373 / ASTM-C20
CeramTec Rubalit® 710 Alumina, 99.6%
Rubalit® 710 (99.6%) is an alumina that produces optimum results and is considered the material of choice for thin-film technology. Its characterizing features are high strength and thermal conduct..
Density 3.90 g/cc
0.141 lb/in³
DIN EN 623-2
CeramTec V 679 Alumina, 99.7%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.
Density 3.90 g/cc
0.141 lb/in³
ASTM-C 20
CoorsTek AD-996 99.6% Alumina
Density 3.90 g/cc
0.141 lb/in³
ASTM-C373
CoorsTek ADS-995R MidFilm™ 99.5% Alumina Thick Film
Applications: thick films and lasers
Density 3.90 g/cc
0.141 lb/in³
ASTM-C 20
CoorsTek CAP 3 99.5% Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
Density 3.90 g/cc
0.141 lb/in³
BASF Paliotan® Yellow L 1145 Color Additive
Description: Pigment combination based on Bismuth VanadateSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, and Airdrying systems.Information provided by BASF
Density 3.90 g/cc
0.141 lb/in³
ISO 1183
Azoty Tarnow™ TARFLEN SM-B60 PTFE
Tarflen SM1 reinforced with 60% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Density >= 3.90 g/cc
>= 0.141 lb/in³
Advanced Ceramics ACL 1091 (C-799) Alumina