Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.134 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 3.70 - 3.75 g/cc
0.134 - 0.135 lb/in³
Sintered
Nabaltec GRANALOX® NM 9510 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Density 3.70 - 3.80 g/cc
0.134 - 0.137 lb/in³
Sintered Density
Nabaltec GRANALOX® NM 9612 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Density 3.70 - 3.75 g/cc
0.134 - 0.135 lb/in³
Sintered Density
Nabaltec GRANALOX® NM 9620 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Density 3.70 - 3.80 g/cc
0.134 - 0.137 lb/in³
Sintered Density
Nabaltec GRANALOX® NM 9620 F Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Density 3.70 g/cc
0.134 lb/in³
Sintered Density
Nabaltec NABALOX® NO 325 Ground Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.70 g/cc
0.134 lb/in³
Sintered Density
Nabaltec NABALOX® NO 615-10 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.70 g/cc
0.134 lb/in³
Sintered Density
Nabaltec NABALOX® NO 625-10 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 3.70 g/cc
0.134 lb/in³
NanoScale NanoActive® Titanium Dioxide
NanoActive TiO2 is produced using proprietary processes to obtain high specific surface area (over 500 m²/g), high porosity, weakly aggregated, amorphous material possessing adsorption capacity and..
Density 3.70 g/cc
0.134 lb/in³
MarkeTech Repton EXP 383 Alumina 96%
REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa..
Density 3.72 g/cc
0.134 lb/in³
GBC Grade 97 Alumina
Data provided by the manufacturer, GBC Materials Corporation.
Density 3.70 g/cc
0.134 lb/in³
Misumi Alumina 96 Aluminum Oxide, Al2O3
Information provided by MISUMI Corporation.
Density 3.71 g/cc
0.134 lb/in³
Indium Corp. Indalloy 186 Germanium-Aluminum Solder Alloy
Information Provided by Indium Corporation
Density 3.70 g/cc
0.134 lb/in³
Schott N-PK52A Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
Density 3.71 g/cc
0.134 lb/in³
Schott N-SSK5 Glass
Information Provided by SCHOTT North America, Inc.
Density 3.70 g/cc
0.134 lb/in³
ASTM D792
Techmer ES Electrablend® PPS 06000
Availability: North AmericaForms: PelletsFiller/Reinforcement: Metallic FlakeFeatures: Electrically ConductiveInformation provided by TP Composites, Inc.
Density 3.70 g/cc
0.134 lb/in³
Sapco 95% Aluminum Oxide
Information provided by Sapco.
Density 3.70 g/cc
0.134 lb/in³
CeramTec Rubalit® A 1894 Alumina, 94%
Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond ..
Density 3.70 g/cc
0.134 lb/in³
ASTM C20
CoorsTek AD-94 Alumina (nom. 94% Al2O3)
Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Density 3.72 g/cc
0.134 lb/in³
ASTM-C373
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate
This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers
Density 3.70 g/cc
0.134 lb/in³
ASTM-C 20
CoorsTek Z-PLUS™ 94 Zirconia-Impr. Alumina Ceramic Armor Material
CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys..
Density 3.70 g/cc
0.134 lb/in³
Du-Co Ceramics DC-265-L-6 Alumina, 96% Al2O3
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Density >= 3.70 g/cc
>= 0.134 lb/in³
Advanced Ceramics ALC 1082 (C-786) Alumina
Information provided by Advanced Ceramics Limited (ACL)
Density 3.70 g/cc
0.134 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon R36580N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat..
Density 3.70 g/cc
0.134 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon Thermabond® 99730N004 0.004" (0.102 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Electrically Conductive - Thermabond®. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Coring..
Density 3.70 g/cc
0.134 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon Thermabond® 99730N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Electrically Conductive - Thermabond®. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Coring..
Density 3.70 g/cc
0.134 lb/in³
DIN EN 623-2 / ASTM-C373 / ASTM-C20
CeramTec 614/698 Alumina, 96%
614/698 (96%) is a high-strength alumina with good mechanical properties, as well as good wear and chemical resistance. It also features excellent electrical properties. 614 is white; 698 is pink.
Density 3.72 g/cc
0.134 lb/in³
DIN EN 623-2
CeramTec Rubalit® IS 95 Brown Alumina
Rubalit® IS 95 brown is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at..
Density 3.70 - 4.40 g/cc
0.134 - 0.159 lb/in³
ASTM B417
H.C. Starck Amperit® 551.059 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni)
Density 3.70 - 4.40 g/cc
0.134 - 0.159 lb/in³
ASTM B212
H.C. Starck Amperit® 551.074 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni)
Density 3.70 - 4.40 g/cc
0.134 - 0.159 lb/in³
ASTM B212
H.C. Starck Amperit® 551.088 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni)
Copyright © lookpolymers.com All Rights Reserved