Indium Corp. Indalloy 186 Germanium-Aluminum Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 186 Germanium-Aluminum Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 3.71 g/cc
0.134 lb/in³
Thermal Properties Metric English Comments
Melting Point 424 °C
795 °F
Eutectic
Solidus 424 °C
795 °F
Liquidus 424 °C
795 °F
Component Elements Properties Metric English Comments
Aluminum, Al 45 %
45 %
Germanium, Ge 55 %
55 %