Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0777 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.15 - 2.25 g/cc
0.0777 - 0.0813 lb/in³
ASTM D792
Polikim EFALON® C-15 PTFE, 15% Glass Filled
C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings..
Density 2.15 g/cc
0.0777 lb/in³
ASTM D4894
3M Dyneon™ 1620 PTFE Powder  (discontinued **)
Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
Density 2.15 g/cc
0.0777 lb/in³
ASTM D4894
3M Dyneon™ 1641 PTFE Powder  (discontinued **)
Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
Density 2.15 g/cc
0.0777 lb/in³
ASTM D4894
3M Dyneon™ 1645 PTFE Powder  (discontinued **)
Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
Density 2.15 g/cc
0.0777 lb/in³
Sintered moldings; ASTM D4894/D4895
3M Dyneon™ TF 2024 PTFE Paste Extrusion Powder  (discontinued **)
Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 500. Average particle size 500µm. Used for unsintered tapes and sealing cords.Dyneon offers a family of PTFE fine powder ..
Density 2.15 g/cc
0.0777 lb/in³
Sintered moldings; ASTM D4894/D4895
3M Dyneon™ TF 2025 PTFE Paste Extrusion Powder  (discontinued **)
Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 300. Average particle size 500µm. Used for liners.Dyneon offers a family of PTFE fine powder paste extrusion resins. Thes..
Density 2.15 g/cc
0.0777 lb/in³
Sintered moldings; ASTM D4894/D4895
3M Dyneon™ TF 4303 PTFE 15% Graphite Filled  (discontinued **)
Type II PTFE. Applications include sliding surfaces, bearings, seals/gaskets.Data provided by Dyneon.
Density 2.15 g/cc
0.0777 lb/in³
Sintered moldings; ASTM D4894/D4895
3M Dyneon™ TF 4220 PTFE 2% Cond. Pigm. Filled  (discontinued **)
Applications include antistat linings, seals, gaskets, moldings.Data provided by Dyneon.
Density 2.15 g/cc
0.0777 lb/in³
ASTM D4895
3M Dyneon™ TF 2025 PTFE  (discontinued **)
Processable by standard paste extrusion methodsBoth grades can be processed at low to medium reduction ratiosTF 2021 PTFE is preferred for unsintered thread sealing tapes and expanded joint sealants..
Density 2.15 g/cc
0.0777 lb/in³
ISO 12086
3M Dyneon™ TF 2029 PTFE  (discontinued **)
Processable by standard paste extrusion methodsDesigned for low reduction ratiosCan be processed at a high stretch ratiosRecommended for apes requiring high mechanical strength, such as electrical t..
Density 2.15 g/cc
0.0777 lb/in³
ISO 12086
3M Dyneon™ TF 2053 PTFE  (discontinued **)
Processed by standard paste extrusion methodRecommended grade for extrusion of tubing and cables requiring only moderately high reduction ratioGood overall balance of mechanical properties and proce..
Density 2.15 g/cc
0.0777 lb/in³
Sintered Sheets; ISO 12086
3M Dyneon™ TFM™ 2001 PTFE  (discontinued **)
Processable by standard paste extrusion methodRecommended for high performance applications with reduction ratios up to 1000:1Provides denser polymer structure with fewer micro voids and lower gas p..
Density 2.15 - 2.18 g/cc
0.0777 - 0.0788 lb/in³
DIN 53479
Fluorseals PTFE Unfilled
Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Density 2.15 g/cc
0.0777 lb/in³
Apparent
Gouda Vuurvast B 1 Dense Refractory Brick
Description: B 1 is a fireclay quality for general applications up to 1350°CRemarks: This data represents average values, obtained from samples that were cut from standard bricks.Information prov..
Density 2.15 g/cc
0.0777 lb/in³
ASTM D792
ScanTube FEP Tubing
Information provided by ScanTube, Inc.
Density 2.15 g/cc
0.0777 lb/in³
ASTM D792
ScanTube MFA Tubing
Information provided by ScanTube, Inc.
Density 2.15 g/cc
0.0777 lb/in³
ASTM D792
ScanTube PFA Tubing
Information provided by ScanTube, Inc.
Density 2.15 g/cc
0.0777 lb/in³
ASTM D792
ScanTube PTFE Tubing
Information provided by ScanTube, Inc.
Density 2.15 - 2.19 g/cc
0.0777 - 0.0791 lb/in³
BS2782:Pt6
Dalau Dalcon 086 100% Virgin PTFE modified polymer
Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal ..
Density 2.15 g/cc
0.0777 lb/in³
ISO 1183
Azoty Tarnow™ TARFLEN SM-1 PTFE
Non Free-Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Density 2.15 g/cc
0.0777 lb/in³
ISO 1183
Azoty Tarnow™ TARFLEN SM-2 PTFE
Non Free Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Density 2.15 g/cc
0.0777 lb/in³
ISO 1183
Azoty Tarnow™ TARFLEN ST PTFE
Free-Flowing suspension powder for ram extrusion of rods, pipes and other profiles.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Density 2.15 - 2.30 g/cc
0.0777 - 0.0831 lb/in³
Aremco Ceramabond™ 516 High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Density 2.15 g/cc
0.0777 lb/in³
Sintered Sheets; DIN EN ISO 12086
3M Dyneon™ TFM™ 2001Z PTFE
Dyneon™ TFM™ 2001 Z PTFE is an ideal grade for high-performance applications with reduction ratios up to 1000:1. This product has a denser polymer texture providing lower gas permeability than sta..
Density 2.15 g/cc
0.0777 lb/in³
DIN EN ISO 12086
3M Dyneon™ TF 2021Z PTFE Fine Powder
Dyneon TF 2021 Z PTFE is an ideal grade for pipe liner applications because of its outstanding green strength. It is the preferred grade for unsintered thread sealing tapes, expanded join sealings, ..
Density 2.15 g/cc
0.0777 lb/in³
DIN EN ISO 12086
3M Dyneon™ TF 2029Z PTFE Fine Powder
Dyneon™ TF 2029 Z PTFE is an ideal grade for tapes with high mechanical strength, such as electrical tape for wrapped insulations or flat cables. Also ideal for yarn applications, including sewing ..
Density 2.15 g/cc
0.0777 lb/in³
ASTM D792
Solvay Specialty Polymers Algoflon® E2 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Pre Sintered. Type V Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent di..
Density 2.15 g/cc
0.0777 lb/in³
ASTM D792
Solvay Specialty Polymers Algoflon® E2 BP PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Pre Sintered. Type V Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent di..
Density 2.15 g/cc
0.0777 lb/in³
ASTM D792
Solvay Specialty Polymers Algoflon® 1.2CSC PTFE; Superconductive Carbon Filled  (discontinued **)
Data provided by the manufacturer.1.2 wt.% Superconductive Carbon. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric prope..
Density 2.15 g/cc
0.0777 lb/in³
Sintered moldings; ASTM D4894/D4895
3M Dyneon™ TFM™ 4220 Modified PTFE, 2% Cond. Pigm. Filled  (discontinued **)
Applications include antistat linings, seals, gaskets, moldings.Data provided by Dyneon.
Copyright © lookpolymers.com All Rights Reserved