Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792 |
Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792 |
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Density | 2.00 - 2.30 g/cc | 0.0723 - 0.0831 lb/in³ | Average value: 2.16 g/cc Grade Count:35 |
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ISO 1183 |
Hexion Bakelite™ PF 1107 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures
(disconti Phenolic molding compound, inorganically filled, glass fiber reinforced, high heat resistance, low heat expansion coefficient, highest resistance to pressure, high dimensional stability.Application .. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 1500 Unsaturated Polyester UP BMC 1500 is a special BMC for the use at elevated temperature. The glass content is set to a level that combines good flowability with good strength and stiffness properties. Even without a specific.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792 |
Glastic Laminates/Shapes MTS Grade MTS Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 3000 Unsaturated Polyester UP BMC 3000 is a special BMC suitable for the use in microwave and cookware applications.It has high temperature resistance, and meets requirements for food contact applications. It has a high gloss fi.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 3100 Unsaturated Polyester UP BMC 3100 is a special BMC suitable for the use in head lamp reflectors. Because of its high temperature resistance and dimensional stability as well as low coefficient of thermal expansion, complex .. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ryton® R-7-190BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-190BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical .. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ryton® R-7-190NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-190NA glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical .. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | |
Specialty Materials 5521 Boron Epoxy Prepreg Tape Specialty Materials' 5521 is a highly advanced prepreg tape, combining Specialty Materials' 4.0 or 5.6 mil boron filament with a tough, rigid, epoxy resin. Performing at temperatures up to 350°F,.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | |
Saint-Gobain Chemfab® 10 Industrial PTFE-Coated Glass Description: Chemfab® Industrial Series products are multi-purpose, non-porous, medium-resin content, PTFE-coated fiberglass fabrics. Applications include release sheets, packaging, composites, g.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792 |
Plastics Group Polifil® BS-70 70% Barium Sulfate Reinforced Polypropylene Polifil® BS series compounds are homopolymer polypropylene resins reinforced with barium sulfate. They possess increased specific gravity, high flex modulus, high deflection temperature, good chemi.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | |
Cosmic Plastics CP7311 Epoxy Molding Compound Data provided by the manufacturer. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | |
Cosmic Plastics CP7318 Short Glass Fiber Filled Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM F1315 |
Thermoseal KLINGERSIL® C-4409 Metal Reinforced Gasketing Synthetic FiberNitrile BinderHigh Temperature & StressExcellent in Hot GasesReplaces Spiral WoundsVibrationGalvanized Low Carbon Steel InsertInformation provided by Thermoseal Inc. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | Cured |
Chesterton ARC 10 Paste grade machinable composite Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance and corrosion resistance. It is non-sag.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | |
Du-Co Ceramics DC-142 Aluminum Silicate Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | Filament Property. |
Cytec Thornel® Mat VMC Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Prepared by sectioning mat VMA into cubes ~ 0.5x0.5x1.0 in. VMC can be heterogeneously dispersed in matrix materials and thus enha.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ISO 1183/A |
Addiplast Addilene J 522 K20 Polypropylene Copolymer High densityInformation provided by Addiplast. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | |
3M Dyneon™ PFE 133TBZ High Temperature Perfluoroelastomer 3M™ Dyneon™ PFE 133TBZ is a technically advanced high temperature perfluorelastomer (HT PFE). It is designed to meet the challenges of higher temperature plasma applications. It is classified as F.. |
|||
Density | 2.00 - 2.15 g/cc | 0.0723 - 0.0777 lb/in³ | |
Aremco Ceramabond™ 835-MB High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792A |
Resinoid 1320 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792A |
Resinoid 1323 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792 |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 50 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |