Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE G 7155 BLK Multi-Flex® G 7155 is based on Shell's Kraton G technology, manufactured under the license of Shell. Multibase certifies that his product has been formulated with the same ingredients as manufactu.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | Green Density |
Nabaltec NABALOX® NO 113 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | |
Premix Thermoplastics PRESEAL® TPE 6070 PRESEAL TPE 6070 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasketing and grounding applications. Conductivity is achieved with a silver coated glass sp.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | |
3M Dyneon™ Fluorel™ FLS-2530 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 69%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. High fluorine dipolymer with improved f.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | |
Cookson Group Plaskon® 3100LS Mineral Filled Conventional Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A semiconductor grade encapsulant suitable for a wide range of applications ranging from small SOICs to moderate lead count DIPs... |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D792 |
G-9 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-9 has high arc and heat resistance and is recommended for humid environments. It is used for switch board pane.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | |
Haveg 41N Phenolic; Silicate Reinforced Ablative Material A proprietary thermoset plastic consisting of a phenol-formaldehyde resin and non-asbestos silicate fillers converted to a permanent thermoset state under heat and pressure. It is designed for abla.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D572 |
Haysite 14200 Polyester BMC, 15% Glass Reinforced The 14200 series bulk molding compound is one of Haysite's newest molding compound families. This grade can be compression, transfer, or injection molded. Good mechanical strength and exceptional a.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | |
SGL Carbon Group EK 2230 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | |
SGL Carbon Group V 1626 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® M30 PFPE Lubricant Information provided by Solvay Solexis, Inc. |
|||
Density | 1.85 g/cc @Temperature 25.0 °C |
0.0668 lb/in³ @Temperature 77.0 °F |
|
Solvay Specialty Polymers Galden® HT270 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP UFW49S PPA LNP* THERMOCOMP* UFW49S is a compound based on Polyphthalamide resin containing 45% Glass Fiber, 20% Wollastonite. Added features of this material include: Heat Stabilized, Low Warpage. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D792 |
Plenco 08235 Polyester BMC, Compression Molded PLENCO 08235 is a renumber of PlasGlas 20315. PLENCO 08235 is a 15% glass-filled polyester bulk molding compound characterized as a flame-retardant, medium strength electrical grade. It is suitable .. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D792 - ISO 1183 |
DuPont Keldax® 6705B Filled Thermoplastic Ethylene Polymer A filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications.Processing Method: ExtrusionSheetAvailability: Nor.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | |
Cosmic Plastics E486 lass Filled Epoxy Molding Compound, Electrical Grade Data provided by the manufacturer. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | |
Cosmic Plastics E487 lass Filled Epoxy Molding Compound, Electrical Grade Data provided by the manufacturer. |
|||
Density | 1.85 g/cc @Thickness >=0.000 mm |
0.0668 lb/in³ @Thickness >=0.000 in |
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 61212-2 7.3 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Tubes Description: Mechanical and electrical applications. High mechanical strength. Self-extinguishing, halogen-free. Good resistance to chemicals.Information provided by Elektro-Isola |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 |
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GF45 NL PBT 45% filled, high gloss, increased density Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 |
Elektro-Isola G-Etronax EP 203 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NAX0 GR70 NL HS PA6.6, 70% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon Thermabond® 99A90X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Density | 1.85 - 2.10 g/cc | 0.0668 - 0.0759 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATR 457© Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:High shock resistant ( high impact strength ) High Mechanical StrengthHigh Dielectric StrengthHigh Electrical Insulation Color- pale brown Medium flow Applications:Electric motor en.. |
|||
Density | 1.85 - 2.05 g/cc | 0.0668 - 0.0741 lb/in³ | Molded |
Bulk Molding Compounds BMC T15(F) High Strength Grade Molding Compound BMC T15F is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15F is well suited for injection, transfer or compression molding.. |
|||
Density | 1.85 g/cc | 0.0668 lb/in³ | ASTM D792 Method A |
Arlon 45N Multifunctional Epoxy Laminate and Prepreg Arlon 45N is a tough, high Tg (175°C by DSC) multifunctional epoxy laminate and prepreg system designed for use in a variety of higher layer count MLBs. Processable using conventional FR-4 conditi.. |
|||
Density | 1.85 - 2.30 g/cc | 0.0668 - 0.0831 lb/in³ | Compounded |
Fluorocarbon Rubber (FPM), Low Temperature Grade Fluorocarbon rubbers are very stable toward degradation by chemicals, heat, and oxidation. Some chemicals that attack FPM include ketones, low molecular weight esters, and nitrogen containing solve.. |