Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
LNP Lubricomp® EFL-4036 UFE Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | |
IDI Composites M-209 Thermoset Polyester, Sheet MECHANICAL - Versatile family of compounds designed to meet a variety of mechanical, electro-mechanical, and corrosion applications. Outstanding structural properties at lowest possible costs.Data p.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | |
LATI Latamid 6 H2 G/55 PA 6, 55% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Asia Pacific) LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Europe-Africa-Middle East) LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36XXC PEI LNP* Lubricomp* EFL36XXC is a compound based on Polyetherimide containing 30% Glass Fiber, 155 PTFE. Characteristics of this grade are: Internally Lubricated. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36XXC PEI LNP* Lubricomp* EFL36XXC is a compound based on Polyetherimide containing 30% Glass Fiber, 155 PTFE. Characteristics of this grade are: Internally Lubricated. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PBT GF30 FR-S AS 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: AntistaticFeatures: Flame Retardant, Antistatic and Non-BloomingProcessing Method: Injection.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
Techmer ES HiFill® ABS GF60 LE 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6/6 GF30 FR HS2 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Asia Pacific) Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Asia Pacific) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | dry; ISO 1183 |
DSM Stanyl® 46HF4550 PA46-GF50 50% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | dry; ISO 1183 |
DSM Stanyl® OCD2300 BLK PA46-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | dry; ISO 1183 |
DSM Stanyl® TC153 PA46 FR(17) Thermal conductive material, Flame Retardant, Heat Stabilized |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 BK010 is a 30% mineral reinforced flame retardant black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
Barlog Plastics KEBAFLOW HF130 LCP, 30% glass fiber reinforced LCP-GF30Information provided by BARLOG plastics GmbH. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Density | 1.62 g/cc @Temperature 23.0 °C |
0.0585 lb/in³ @Temperature 73.4 °F |
ASTM D792 |
Beijing Ranger Chem PBT 403 M-G30 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ASTM D792 |
Chem Polymer Durlex 730 GVH PBT, 30% Glass Fiber Reinforced A glass fiber reinforced, flame retardant PBT exhibiting excellent strength, dimensional stability and elevated temperature performance. The material has a V0 flammability rating according to UL94 .. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP JF006E PES (Europe-Africa-Middle East) LNP* Thermocomp* JF006E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183/A |
Addiplast Addinyl B2H M30 Flame Retardant Nylon 6, 30% Mineral Filled Flame retardant, 30% mineral filled, with halogensInformation provided by Addiplast. |