Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
PolyOne Nymax™ GMF 604 40 UV Black 115 1 X 1 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | |
Nylene® PA6/6 Glass/Mineral Filled 7215 HS Nylon 6/6 15% Glass Reinforced/25% Mineral Filled.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
Owens Corning Glass Fiber Reinforced Nylon 6/6, 30 wt.% glass Nylons, as a group, are inert to most organic solvents. They resist alkalis and salt solutions and they are attacked by strong mineral acids and oxidizing agents. Data provided by the manufacturer,.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
Polykemi AB SCANBLEND P AP2060 F30 PBT/ASA, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
Polykemi AB SCANTEC PC S60R GF30 V0 Polycarbonate, Glass-Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
Covestro Petlon® DP3-1039 Semi-Crystalline PET, 35% Glass Fiber
(discontinued **) Characteristics: Impact Modified: Good Strength and ToughnessApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperature: 495-530°F, Mold Tempe.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
Nilit FRIANYL C73 MG40 Nylon 6.6/6 for injection molding, 40% mineral filled Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
LATI LATAN 13 K/30 30% Carbon Fiber Reinforced Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® S223-G8U (Cond.) 43% Glass Reinforced Nylon 66 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | |
Momentive Performance Materials RTV60 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | |
LATI Latilub 66-15T G/30 PA66, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP KP004 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KP004 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP KP004AXP POM (Europe-Africa-Middle East) LNP* LUBRICOMP* KP004AXP is a compound based on Acetal Homopolymer containing PTFE, Silicone. Added features include Internally Lubricated. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP KP004XXP Acetal Copolymer LNP LUBRICOMP* KP004XXP is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp RFM62 PA 66 LNP* Lubricomp* RFM62 is a compound based on Nylon 66 resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 LNP* LUBRICOMP* RFP36 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE, Silicone. Added features of this material include: Wear Resistant. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
Techmer ES Elastoblend® PA6 GF43 IM L BKN 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
Sax Polymers SAXAMID 126F4MW4 Nylon 6, 40% Glass Fiber and Mineral Reinforced SAXAMID 126F4MW4 is a 40% glass fibers/ mineral reinforced polyamide 6 injection-molding-grade. It has dimensional stability and high strength.Information provided by SAX Polymers |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT (Asia Pacific) LNP* Stat-loy* WF306C is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: Antistat, Clean Compounding System. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | GB/1033 |
Zhejiang Juner PA66-301-G20 Flame-Retardant & Glass Reinforced, Environmental PA66 Applications: Framework of CoilsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® XT-5038-9 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® S223-HM8 (Cond.) 40% Mineral Reinforced, Heat Stabilized Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 87/T Flexible PVC, Sheathing Sheath antiroditor - antitermite |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 045/11 Halogen Free PVC Sheathing; designed to meet VDE 0207 part 24 HM4 |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 3622 Halogen Free PVC General purpose |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
Ascend Performance Materials Vydyne® R228 Nylon 66, 40% Mineral Reinforced, Conditioned Vydyne® R228 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in black, it is an injection-molding grade formulated to retain the inherent processing advant.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
Plenco 4485 Phenolic, Granular, Transfer Molded PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a.. |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 50/C Flexible PVC, Extrusion Gaskets for frames |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
Plenco 51015 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by.. |