Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | 11.6# part A, 8.8# part B |
Abatron KromaKote 8901-8 Polyurethane Coating
(discontinued **) 2-component system for outstanding performance in normal, industrial, marine and corrosive environments. Superb combination of chemical, solvent, abrasion and weather resistance.Suggested Uses: Pro.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® ML3019 PC (Europe-Africa-Middle East) LEXAN ML3019 is a medium viscosity, 10% glass reinforced, flame retardant grade, especially designed for applications like industrial enclosures and fuse boxes requiring a low knock-out strength for.. |
|||
Density | 1.27 - 1.57 g/cc | 0.0459 - 0.0567 lb/in³ | Average value: 1.40 g/cc Grade Count:31 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | |
Lord Adhesives 309 General Purpose, Non-Sag, Thixotropic Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem 1010FV PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem 1010KM PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem 1010RV PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas r.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem 1100V PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP RX85514 PA 66 (Asia Pacific) LNP* LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA 12 (Asia Pacific) LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conductive. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP UX06002 PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UX06002 is a compound based on Polyphthalamide resin containing Aramide Fiber, PTFE. Added features include: Easy Molding, Internally Lubricated, Heat Stabilized. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem HATX200 PEI+PCE High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM HU1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem HU1000E PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
Teijin Multilon DN-3510F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 10 % filler. Improved stiffness and high fluidity realizes a thin wall.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183B |
Styron CALIBREâ„¢ 7103-8 Polycarbonate CALIBREâ„¢ 7103-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, Conditioned Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM AUT200 PEI Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperat.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON RE006 PA6.6 (Asia Pacific) LNP STAT-KON RE006 is a compound based on Nylon 66 containing carbon fiber. Added features of this material include: Electrically Conductive. Also known as STAT-KON RC-1006 |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
Polyram PlusTek PA340S4 Nylon 66 for Injection Molding, 20% Glass-Beads Reinforced 20% Glass-beads reinforced Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
Eurostar Starglas CF006 Styrenic, 30% Glass Filled, Injection Molding Starglas CF006 is a 30% Glass Fiber Reinforced Styrenic Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NA40 GR20 NL HS PA6.6, 20% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NB30 GR13 BK EF PA6, 13% glass fiber reinforced, black, suitable for electrostatic powder coating Information provided by Eurotec® |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ISO 1183 |
Akro-Plastic Akromid® B3 GF 20 (2470) PA 6 Conditioned, 20% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | ASTM D 792 |
API Megol AM DP2154 SEBS Adhesion Modified Overmolding for PA Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | |
A. Schulman ComAlloy Hiloy® 637 Nylon 6/6, Glass/Mineral Reinforced, Flow Enhanced, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.27 g/cc | 0.0459 lb/in³ | dry; ISO 1183 |
DSM Novamid® 3010CF30 BK PA66-CF30 30% Carbon Reinforced |