Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
PolyOne OnFlex™ HT 40A-3S2131 Thermoplastic Elastomer (TPE) OnFlex™ HT thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds is specially formulated to deliver very good compression set performance at.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PP CQX15015 R3 UV Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | TPE-0105 (ASTM D792) |
ExxonMobil Vyram™ 9271-55 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Hybrid Plastics CO6U50.01 Nanoreinforced® Cyclic Olefin Copolymer Impact modified, UV stabilizedThe exceptional heat distortion temperature and low density of cyclic olefin copolymers (COC) makes them excellent materials for high temperature applications where low.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | Not Compounded |
KKPC Kumho KHS 65 High Styrene Resin Masterbatch (HSR) High Styrene Resin Masterbatch (HSR)Characteristics: KOSYN KHS is produced by mixing SBR 1502 of 23.5% styrene and high styrene resin latex at high temperature. It works as plasticizer which improve.. |
|||
Density | 1.00 - 1.10 g/cc | 0.0361 - 0.0397 lb/in³ | 2.4% Lucolast in Bitumen B50/70 |
Lucobit Lucolast® 7010 Ethylene Butyl Acrylate Asphalt Additive Lucolast® 7010 is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Addition of Lucolast 7010 to bitumen increases its viscosity, broadens the range of plasticit.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | As Supplied |
Heraeus Cleviosâ„¢ P HC V4 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P HC V4 is an antistatic material based on PED.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | Not Compounded |
KKPC Kumho KHS 68 High Styrene Resin Masterbatch (HSR) High Styrene Resin Masterbatch (HSR)Characteristics: KOSYN KHS is produced by mixing SBR 1502 of 23.5% styrene and high styrene resin latex at high temperature. It works as plasticizer which improve.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
LATI Latistat 47/7-03 PP Copolymer Dissipative product based on Polypropylene copolymer (PPc). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ASTM D792 |
Techmer ES Electrafil® PP-61/EC Copolymer Polypropylene, Conductive Carbon Filled Conductive Carbon, Powder Modified |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp M10009A PP (Europe-Africa-Middle East) LNP* STARFLAM* M10009A is a compound based on Polypropylene resin, containing Flame Retardant. Added features include : Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middl.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Solvay ALKAMULS® AP Surfactant Description: Ethoxylated oleic acid with low free PEG contentIdentification: ETHOXYLATED OLEIC ACIDCAS: 9004 – 96 – 0Available in: Asia Pacific, Europe, Latin America Solubility: Dispersib.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Solvay ALKAMULS® PSTO 20 Surfactant Description: Good emulsification characteristics, particularly in combination with high or low HLB surfactants to form W/O or O/W emulsions.Chemical Name: ETHOXYLATED SORBITAN TRIOLEATECAS: 9005-70-.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP M7002XXH PP LNP* THERMOCOMP* M7002XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additives. Designed for touch surfaces in healthcare applications. Added features include:.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ASTM D792 |
Washington Penn High Modulus Polypropylene Copolymer 15% Mica Filled Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Trelleborg Emerson & Cuming Eccobond® 9 General Purpose Catalyst Emerson & Cuming 9 Eccobond® General Purpose CatalystGeneral purpose, low viscosity. Imparts good physical strength and chemical resistance to cured castings. Recommended for most general purpose a.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ASTM D792 |
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
Polyram RamOfin PPH300G3 Polypropylene, 15% Glass Fiber 15% Glass fiber reinforced polypropylene for injection molding application.Information provided by Polyram. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Dow Corning SYL-OFF® PMCPSL 7 Crosslinker Minimizes mist at speeds up to 1600 m/min, good anchorage to and stability with many paper substrates, suitable for lamination with a variety of adhesives.Information provided by Dow Corning |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Dow Corning SYL-OFF® PMCPSL 8 Crosslinker Syl-Off SL 8 Crosslinker is very fast cure (contains mist reduction additive)Information provided by Dow Corning |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Dow Corning SYL-OFF® PMCPSL 9176 Anchorage Additive Syl-Off® SL 9176 Anchorage Additive is one component of a multi-component silicone release system designing for coating on film substrates.Information provided by Dow Corning |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Eliokem Chemigum® P8BA Nitrile Elastomer High melt strength. Particularly recommended for extrusion and calendaring. 33% bound ACN. Branched crosslinked polymer structure. PVC partitioning agent.Can be used in PVC blends.Used in automo.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® TR 90 PAMACM12 Product description: Grilamid TR 90 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 natural offers outstanding properties.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ASTM D297 |
Dow Nordel® NDR 37060.02 EPDM Hydrocarbon Rubber Description: NDR 37060.02 is a medium viscosity, medium ethylene EPDM grade having a moderate cure rate that is suited to applications where low modulus, good elongation, as well as heat and weather.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
Arkema Group Pebax® 2533 SD 02 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 2533 SD 02 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SD grade is heat and UV stabilized and contains mold release additive.Infor.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ASTM D792 |
Beijing Chemical Industry KAIFA® GL2100 ABS Good Flow Grade Good flow, Easy processing, High glossInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Density | 1.00 - 1.51 g/cc | 0.0361 - 0.0546 lb/in³ | Average value: 1.22 g/cc Grade Count:44 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |
|||
Density | 1.00 - 1.51 g/cc | 0.0361 - 0.0546 lb/in³ | Average value: 1.14 g/cc Grade Count:288 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |