Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.978 g/cc | 0.0353 lb/in³ | |
NEU NeuSoft™ 597-50A Industrial Ether TPU / SBC blend |
|||
Density | 0.978 g/cc | 0.0353 lb/in³ | ASTM D792 |
North Wood Plastics 60 PP + UNIFILL (20% Wood Fiber) Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It.. |
|||
Density | 0.978 g/cc @Temperature 20.0 °C |
0.0353 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell Glycol Ether DBA Diethylene glycol butyl ether acetate Information provided by Lyondell. |
|||
Density | 0.977 - 1.013 g/cc | 0.0353 - 0.03660 lb/in³ | |
Lord Adhesives Flocklok® 853 Blocked Flock Adhesive Flocklok® 853 is a blocked, heat-curing, single coat adhesive used to adhere polyester or nylon fibers (flock) to a variety of elastomers including EPDM, NR, CR, and SBR. Flocked substrates provi.. |
|||
Density | 0.977 g/cc | 0.0353 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA420FS Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, very fast curing.Information provided by Illinois Tool Works. |
|||
Density | 0.976 g/cc | 0.0353 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Density | 0.976 g/cc | 0.0353 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific) LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Density | 0.976 g/cc | 0.0353 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific) LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Density | 0.976 g/cc | 0.0353 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE LNP* STAT-KON* FX98500C is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Density | 0.978 g/cc @Temperature 15.6 °C |
0.0353 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil Exterex™ TM111 Synthetic Fluid Product Description: Esterex™ Tirmellitate Esters are API category Group V fluids. These esters have excellent low-temperature properties, good lubricating properties and low volatilities. Esterex™.. |
|||
Density | 0.976 - 0.982 g/cc | 0.0353 - 0.0355 lb/in³ | BRCP 4843 |
ExxonMobil Jayflex™ TINTM Plasticizer Appearance: Clear and FreeAvailability: North AmericaCAS Number: 53894-23-8Information provided by ExxonMobil |
|||
Density | 0.976 g/cc | 0.0353 lb/in³ | |
BASF 1-Ethynyl-1-cyclohexanol Formula: C8H12OCAS: 78-27-3Description: Ethynylcyclohexanol is a colorless solidified mass, with a faint specific odor.Synonyms: 1-EthynylcyclohexanolApplications: Intermediate used in the productio.. |
|||
Density | 0.977 g/cc | 0.0353 lb/in³ | |
BNZ Materials 2861LI Insulating Aggregate BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i.. |
|||
Density | 0.977 g/cc | 0.0353 lb/in³ | Fired at 5 hrs at 816°C |
BNZ Materials Bazelite 2300 LI Insulating Castable Blaz 2300 L is similar to Blaz 2300 but suitable for those applications where reducing conditions might be encountered. These high purity, low iron products are specifically designed for both back-u.. |
|||
Density | 0.978 - 1.11 g/cc | 0.0353 - 0.0401 lb/in³ | Average value: 1.05 g/cc Grade Count:9 |
Overview of materials for Silicone Polyurethane, Ether Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value.. |