Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D792 |
Polimeros Mexicanos Rotolene® 93835-TG Medium Density Polyethylene MDPE Copolymer with UV8 stabilizer in natural and colors.Recommended for rotomolding. Used for manufacture of water tanks > 2000 liters, cisterns, farm tanks, or tanks to contain strong acids and b.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Polimeros Mexicanos Rotolene® Industrial Black Linear Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene grade which is fully UV8 stabilized. High quality Polyethylene compounded in black, formulated for rotational molding applications requiring excel.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® TI-0338-A MDPE Masterbatch Resin Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ExxonMobil Method |
ExxonMobil OPTEMA™ TC 115 Molding, extrusion and compounding resin
(discontinued **) OPTEMA TC 115 is an ethylene methyl acrylate copolymer, which can be used as a compatibilizer and impact modifier for engineering thermoplastics. It has been processed at temperatures up to 625°F w.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D4883 |
ExxonMobil LL 8450 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. This resin is ideally suited for applications that require optimum balance.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9640 HDPE Blown Film Resin
(discontinued **) Copolymerization Enhances Film Toughness, Unique Combination of Density and Melt Index, Excellent Strength Properties as well as Good Heat Seal, Lower Density Imparts a Softer Feel and Lesser Tenden.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Eastman 5223 LDPE 6% VA Copolymer, High Clarity, Ultra-High Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent impact strength, Good heat seal characteristics, High antiblock, No Slip, Good processability. Slip 0 ppm. Antiblock 5000 ppm.Applications:Ice ba.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 8405 UV8D, 8405G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Good ESCR, high impact strength.Applications: Spray tanks.Data provided by the manufacturer. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 115-1653 LMDPE Rotational Molding Resin Description: ICORENE 115-1653 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D4883 (Natural) |
Ineos G36-10-150 HDPE G36-10-150 is a medium density hexene copolymer polyethylene resin designed for the blown geomembrane sheet process. This resin is especially well suited for the production of textured geomembranes... |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® FB/FL 20 HDPE Made for tubular film and special applications.Information provided by Unipetrol RPA |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ISO 1183 |
Total MDPE HL 323 Medium Density Polyethylene, Film Resin Medium molecular weight, medium density film resinCharacteristics:Excellent balance of stiffness and impact strengthGood puncture resistanceExcellent compatibility with LDPE and LLDPEGood tensile st.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D792 |
DuPont Appeel® LSR20D745 Lidding Sealant Resin Appeel® LSR20D745 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperatu.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® HHM TR-130 MDPE Film Resin Medium density resin provides overall balance of tensile, impact, and tear properties in film. It is suited for merchandise, produce, and trash bags. Processing performance is excellent on high st.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer Benefits: good processability, excellent melt strength, broad fusion range, outstanding stress cracking resistanceApplications: geomembrane, gas and chemical containment liners, landfill linersInfor.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® K307 MDPE Hexene Copolymer Extrusion grade hexene copolymerCharacteristics: good processability, excellent melt strength, broad fusion range, outstanding stress crack resistance, meets the requirements of GRI-GM13. Meets A.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 15019CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 15019CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications: Hot.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Appeel® 22D843 Ethylene Acrylate DuPont™ Appeel® 22D843 is a polypropylene modified ethylene acrylate resin designed to function as a masterbatch to achieve peelability in polypropylene based sealant layers. It provides peelable .. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LLP 8450.31 Linear Low Density Polyethylene Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D4883 |
ExxonMobil LLP8450.31 Rotational Molding Resin LProduct Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that requir.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | |
Dow Primacor® 1430 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ FL 01418 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 01418 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. FL 01418 is an excellent sealing materi.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | |
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | |
Dow Primacor® 1420 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM-D792 |
Braskem LH537 LLDPE Cast Film Extrusion Polyethylene LH537 is a LLDPE Hexene produced by Braskem. It offers an excellent processability, stiffness, and soft touch for flat die films. It has very low gel contents. It contains slip absent and antiblock .. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM-D1505 |
Braskem RC35U4 LLDPE Rotomolding Polyethylene The resin RC35U4 is a linear low-density polyethylene, 1-butene based, with high stiffness and an adequate balance of processability and environmental stress cracking resistance. It contains long te.. |
|||
Density | 0.939 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Bapolene® 3039U Polyethylene, Rotational Molding Grade Bapolene 3039U is a hexene linear low density polyethylene designed to provide superior impact resistance. It contains a UV-stabilization package and complies with US FDA 21CFR177.1520.Applications.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D4883 |
ExxonMobil LL 8460 Rotational Molding Resin
(discontinued **) LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require optimum balance of stiffness, processabili.. |