Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin Features: Excellent tensile properties, excellent impact toughness, outstanding gloss and clarity, excellent processability.Applications: Coating and sheathing.Data provided by the manufacturer. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film The Trithene® TS 4016 resin is a mixture of low-density polyethylene (LDPE) with linear low-density polyethylene (LLDPE) designed to meet the needs of the technical films segment for the use of aut.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D 4883 |
Eastman 1810A Polyethylene
(discontinued **) Polyethylene 1810A contains no additives. It is suggested for injection molding applications.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to West.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D4883 |
Eastman 1810F Polyethylene
(discontinued **) Polyethylene 1810F is a fractional-melt low-density formulation with no slip or antiblock. It is suggested for film applications requiring high impact strength, high tear strength and very good opt.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D4883 |
Eastman E6838-964F Polyethylene
(discontinued **) E6838-964F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ExxonMobil Method |
ExxonMobil LD 135.09 Cast Packaging Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. It is suitable for processing in cast film equipment. Applications include food packaging, light to medium duty bags, and textile packaging.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ISO 1183 |
Total Lacqtene® FB 3010 LDPE blown film
(discontinued **) Low density radical polyethylene made by high pressure autoclave. Advised temperature profile : 180 to 220°C.Information provided provided by Total Petrochemicals.Total Petrochemicals includes form.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Huntsman PE5030 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Good draw down, low neck-in, good heat sealability and adhesion, low smoking, and excellent printabilityApplications: Extrusion: coating grade and general coa.. |
|||
Density | 0.921 - 0.923 g/cc | 0.0333 - 0.0333 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film The Trithene® TX 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and environmental stress cracking resistance (ESCR). Additionally, this product.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Braskem PB 526 LDPE Blow Molding Polyethylene
(discontinued **) Applications: Heavy duty bags; tubes and hoses; shrink films for pallets; tarpaulins. Blown Film. Information provided by Braskem |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ISO 1183 |
FKuR Kunststoff Terralene® LL 1101 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | TSTM 209 B |
Iran Petrochemical (PCC) LH0075 Low Density Polyethylene LH0075 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Applications: carrier bags, shrink film, industria.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA860008 Low Density Polyethylene ApplicationsPETROTHENE NA 860 is a series of medium flow, low density polyethylene resins for the injection molding of caps, closures and other specialty applications. These resins exhibit an excel.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1400HN Powder Ethylene Butyl Acrylate Lucofin 1400HN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN Powder is softer and more flexible than ethy.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
UBE F023 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ISO 1183 |
Borealis FT5232 Low Density Polyethylene FT5232 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes medium slip additive and antioxidant. This grade is developed for the production of packaging film with good op.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | base resin; ISO 1183/ISO 1872-2 |
Borealis LE4201R Polyethylene Insulation Compound, Crosslinkable LE4201R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications LE4201R is intended for insulation of XLPE power cables with rated voltages up.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Westlake EC1924AA Low Density Polyethylene WESTLAKE low-density polyethylene EC1924 is a resin that is widely used in the boardstock coating industry. This material has an excellent combination of low neck-in, ease of processing, good chill-.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Westlake EP413 Low Density Polyethylene WESTLAKE polyethylene EP413 is a low-density polyethylene recommended for blown or cast film clarity applications. This material has very good optical properties, and is suggested for bakery films ,.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ExxonMobil Method |
ExxonMobil LD 105.30 Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 150BW Low Density Polyethylene Resin Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
Dow LDPE 501I Low Density Polyethylene, Clear Film Grade DOW LDPE 501I, a barefoot resin used for bakery film and other packaging applications that require optical clarity. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food con.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
Dow LDPE 586A Low Density Polyethylene, Packaging Grade DOW LDPE 586A resin is used for general purpose packaging applications. It contains medium levels of slip additive and low levels of antiblock additive. This material complies with U.S.FDA regulatio.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
Dow LDPE 640I Low Density Polyethylene, Liner Film Grade DOW LDPE 640I resin is a barefoot general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. This material complies with U.S.FDA regulation 21 CFR .. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D792 |
Dow 959S Linear Low Density Polyethylene (LDPE) DOW Polyethylene 959S is a medium molecular weight distribution homopolymer. This resin has good process-ability over a wide range of molding conditions. Typical applications include lids. It com.. |
|||
Density | 0.923 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Braskem EB 853/72 LDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Lamination film; general purpose; automatic packaging of solids products (FFS). Informatio.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM-D792 |
Braskem LF218/21 LLDPE Cast and Blown Film Extrusion Polyethylene Copolymer LF218/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and optical prope.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Huntsman PE2060 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: High flow characteristics, good processability.Applications: Injection molding: general purpose molding, large moldings including housewares and toys.FDA Note.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Huntsman PE8010 Specialty Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1.. |