Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.705 g/cc | 0.0255 lb/in³ | Dry |
Unifrax Fibermax® Duraboard® 17H Board Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. .. |
|||
Density | 0.705 g/cc | 0.0255 lb/in³ | Dry |
Unifrax Fibermax® Duraboard® 18H Board Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. .. |
|||
Density | <= 0.705 g/cc | <= 0.0255 lb/in³ | |
Engineered Syntactic Systems PSF-42 Polyester Subsea Syntactic Void Filler PSF-42 was developed by Navy subcontractors for simple shipyard-based cavity pours of Naval vessels. This system may be used in any free-flood cavity or void, but is especially valuable in difficult.. |
|||
Density | 0.705 - 0.716 g/cc | 0.0255 - 0.0259 lb/in³ | ASTM D4052 |
ExxonMobil Heptene Appearance: Clear, free of suspended matterInformation provided by ExxonMobil |
|||
Density | 0.705 g/cc | 0.0255 lb/in³ | |
CMT Materials CTB 44 Composite Toolboard High Temperature CTB-44 is manufactured by CMT Materials for a wide variety of vacuum forming applications. It is suitable for use up to 2500F (1210C). CTB-44 utilizes a copolymer base material and smaller cell st.. |
|||
Density | 0.705 g/cc | 0.0255 lb/in³ | |
CMT Materials HYTAC® C Castable Syntactic Tooling HYTAC-C is a one-part castable product in the HYTAC family of syntactics. This product is available as an uncured, single component mixture that may be poured or cast into a wide variety of shapes a.. |
|||
Density | 0.705 - 0.769 g/cc | 0.0255 - 0.0278 lb/in³ | |
CMT Materials HYTAC® FLX Good Durability, Easily Machined & Polished Copolymer Syntactic HYTAC-FLX has been improved for optimum performance in transparent applications. The enhanced formulation is easy to polish and results in minimal to no scratches with transparent sheet materials. .. |
|||
Density | 0.705 g/cc | 0.0255 lb/in³ | ASTM C134 |
BNZ Materials PA 23 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.705 g/cc | 0.0255 lb/in³ | ASTM C134 |
BNZ Materials Zelieblok 2000S Structural Ceramic Insulation Information provided by BNZ Materials Inc. |