Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Density range normally used |
Polimeri Europa Extir® A 3000 AE Expandable Polystyrene, Standard Flame Retardant Particle size range is 0.7 - 1 mm. Minimum apparent density on a discontinuous pre-expander is 15 g/l.Processing technology used for Type A 3000 AE is: Molding, Vacuum.Specific characteristics: DIN.. |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | |
Polimeri Europa Extir® LN 3000 Expandable Polystyrene Extir LN 3000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion.. |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
Polimeri Europa Extir® Verdi VR A3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir Verdi VR A3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not con.. |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
Polimeri Europa Extir® Verdi VR A5000 AE Expandable Polystyrene - Flame Retardant b>Product Description:Extir Verdi VR A5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does.. |
|||
Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Normal range, one pre-expansion |
SABIC EPS 550FF Expandable Polystyrene Product Description: Fire retardant expanded Polystyrene EPS 550FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce.. |
|||
Density | 0.0160 - 0.0250 g/cc | 0.000578 - 0.000903 lb/in³ | Normal range, one pre-expansion |
SABIC EPS 652 Expandable Polystyrene Product Description: Standard expanded Polystyrene EPS 652 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS.. |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
Polimeri Europa Extir® CM Galileo Io 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
Polimeri Europa Extir® CM Galileo Io 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain CFC.. |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
Polimeri Europa Extir® GEO 3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir GEO 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain C.. |
|||
Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | |
Polimeri Europa Extir Leonardo A 3000 AE Expandable Polystyrene
(discontinued **) Extir A 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 3.. |
|||
Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Density range normally used |
Polimeri Europa Extir® A 3000 Expandable Polystyrene, Standard
(discontinued **) Particle size range is 0.7 - 1 mm. Minimum apparent density on a discontinuous pre-expander is 15 g/l.Processing technology used for Type A 3000 is: Molding, Traditional and Blocks.Specific charact.. |
|||
Density | 0.0160 - 0.0300 g/cc | 0.000578 - 0.00108 lb/in³ | Density range normally used |
Polimeri Europa Extir® IA 2000 Expandable Polystyrene, Special Purpose
(discontinued **) Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 15 g/l.Processing technology used for Type IA 2000 is: Molding, Transfer.Specific characteristics: .. |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
Ineos Nova Styrocell® M442C Expandable Polystyrene A high strength, fast cycling regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M4.. |
|||
Density | 0.0160 - 0.0250 g/cc | 0.000578 - 0.000903 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
Ineos Nova Styrocell® M442C Expandable Polystyrene A high strength, fast cycling regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M4.. |
|||
Density | 0.0160 - 0.0250 g/cc | 0.000578 - 0.000903 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 321F Expandable Polystyrene General: Pentfoam 321F is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine and convent.. |
|||
Density | 0.0160 - 0.0170 g/cc | 0.000578 - 0.000614 lb/in³ | |
IRPC Polimaxx Pentfoam 455E Expandable Polystyrene GENERAL: PENTFOAM "455E" IS A SELF EXTINGUISHING (SE) GRADE EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST CYCLES IN VACUUM MOL.. |
|||
Density | 0.0160 g/cc | 0.000578 lb/in³ | 1.2 minute residence time pre-expander |
Jackon JACKOCELL® R312 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ.. |
|||
Density | 0.0160 g/cc | 0.000578 lb/in³ | 2 minute residence time pre-expander |
Jackon JACKOCELL® R411 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionThe unique design of polystyrene chains and additive chemistry in the Jackocell® R411 gives pre-expanded beads of high dimensional stability. The R411 represents the.. |
|||
Density | 0.0160 g/cc | 0.000578 lb/in³ | 75 rpm |
Jackon JACKOCELL® S214 Expanded Polystyrene Construction and Block Molding Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S214 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces a.. |
|||
Density | 0.0160 g/cc | 0.000578 lb/in³ | Based on 65 times expansion |
Samsung Cheil Industries Starex® SG-301 Expandable Polystyrene (EPS) High Expansion Typical Application : Large FloatInformation provided by Samsung Cheil Industries. |
|||
Density | 0.0160 g/cc | 0.000578 lb/in³ | Based on 65 times expansion |
Samsung Cheil Industries Starex® SG-302 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Density | 0.0160 g/cc | 0.000578 lb/in³ | Based on 65 times expansion |
Samsung Cheil Industries Starex® SG-202 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Density | 0.0160 g/cc | 0.000578 lb/in³ | Based on 65 times expansion |
Samsung Cheil Industries Starex® SG-302 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Density | 0.0160 - 0.0480 g/cc | 0.000578 - 0.00173 lb/in³ | |
BASF Styropor® BF 327 EPS Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv.. |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a discontinuous pre-expander |
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does not conta.. |
|||
Density | >= 0.0160 g/cc | >= 0.000578 lb/in³ | Minimum apparent density on a continuous pre-expander after one expansion |
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does not conta.. |
|||
Density | 0.0160 - 0.0170 g/cc | 0.000578 - 0.000614 lb/in³ | |
IRPC Polimaxx Pentfoam 422F Expandable Polystyrene GENERAL: PENTFOAM "422F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V.. |