Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.57 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.11 - 1.57 g/cc
0.0401 - 0.0567 lb/in³
Average value: 1.43 g/cc Grade Count:98
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Density 1.27 - 1.57 g/cc
0.0459 - 0.0567 lb/in³
Average value: 1.40 g/cc Grade Count:31
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Density 1.20 - 1.57 g/cc
0.0434 - 0.0567 lb/in³
Average value: 1.29 g/cc Grade Count:32
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
ISO R 1184
Fainplast Compounds RE 324 Rigid PVC, Extrusion
Furniture profiles
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
ISO R 1184
Fainplast Compounds RE 418 Rigid PVC, Extrusion
Electric channels
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
ISO R 1184
Fainplast Compounds RH 225 Rigid PVC, Antishock Extrusion
Antishock pipes and profiles
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
ISO R 1184
Fainplast Compounds RK 330 Rigid PVC, Extrusion Lead Free
Profiles
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
ISO R 1183
Fainplast Compounds GA 78 Flexible PVC, Flame Retardant Sheathing
General purposes
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
ISO R 1183
Fainplast Compounds GA 80/1 Flexible PVC, Flame Retardant Sheathing
General purposes
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
ISO R 1183
Fainplast Compounds GK 83 Flexible PVC, Flame Retardant Sheathing Lead Free
General purposes
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
ISO R 1183
Fainplast Compounds GK 89 Flexible PVC, Flame Retardant Sheathing Lead Free
General purposes
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
IEC 60811
Fainplast Compounds HAX HF 018/15 Halogen Free PVC
General purpose
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
IEC 60811
Fainplast Compounds HAX HF 019/G Halogen Free PVC
Sheathing; high flexibility
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
IEC 60811
Fainplast Compounds HAX HF 4523 Halogen Free PVC
High flame retardancy
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
ISO R 1184
Fainplast Compounds R 220 Rigid PVC, Extrusion
Rolling shutters
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
ISO R 1184
Fainplast Compounds R 220/R Rigid PVC, Extrusion
Shiny rolling shutters
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
ISO R 1183
Fainplast Compounds CKL 86 Flexible PVC, Sheathing Lead Free
General purposes
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
ISO R 1183
Fainplast Compounds AP 89 Flexible PVC, Flame Retardant Insulation
Power cables
Density 1.53 - 1.57 g/cc
0.0553 - 0.0567 lb/in³
ISO R 1184
Fainplast Compounds RK 225/R Rigid PVC, Extrusion Lead Free
Rolling shutters
Density 1.36 - 1.57 g/cc
0.0491 - 0.0567 lb/in³
Average value: 1.45 g/cc Grade Count:30
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
Density 1.54 - 1.57 g/cc
0.0556 - 0.0567 lb/in³
Average value: 1.56 g/cc Grade Count:5
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi..
Copyright © lookpolymers.com All Rights Reserved