Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.940 - 1.30 g/cc @Temperature 170 - 240 °C |
0.0340 - 0.0470 lb/in³ @Temperature 338 - 464 °F |
Average value: 1.04 g/cc Grade Count:27 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Density | 1.10 - 1.30 g/cc | 0.0397 - 0.0470 lb/in³ | Average value: 1.16 g/cc Grade Count:16 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Density | 0.960 - 1.30 g/cc | 0.0347 - 0.0470 lb/in³ | Average value: 1.05 g/cc Grade Count:13 |
Overview of materials for Polypropylene, Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu.. |
|||
Density | 0.100 - 1.30 g/cc | 0.00361 - 0.0470 lb/in³ | Average value: 0.932 g/cc Grade Count:82 |
Overview of materials for Styrene/Butadiene/Styrene (SBS) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Butadiene/Styrene (SBS)". Each property range of values reported is minimum and maximum values o.. |
|||
Density | 1.20 - 1.30 g/cc | 0.0434 - 0.0470 lb/in³ | DIN 53479/A |
Stanelco Bioplast® GF 106 Biodegradable Plastic Bioplast 106 is a versatile soft product, suitable for blown film extrusion of completely biodegradable products. Many customers find it is a natural replacement for LDPE. Made from potato starch m.. |
|||
Density | 1.20 - 1.30 g/cc | 0.0434 - 0.0470 lb/in³ | FTTC 2443 |
Formosa Plastics 15.5% Sodium Hypochlorite Information provided by Formosa Plastics Corporation, USA |
|||
Density | 1.26 - 1.30 g/cc | 0.0455 - 0.0470 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 008 Flexible PVC, Insulation Insulation |
|||
Density | 1.26 - 1.30 g/cc | 0.0455 - 0.0470 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 65 Flexible PVC, Injection Molding for Footwear Soles - bottom boots |
|||
Density | 1.26 - 1.30 g/cc | 0.0455 - 0.0470 lb/in³ | ISO R 1183 |
Fainplast Compounds FRT 82 Flexible PVC, Insulation Telephone cables |
|||
Density | 1.26 - 1.30 g/cc | 0.0455 - 0.0470 lb/in³ | ISO R 1183 |
Fainplast Compounds PK 0111 Flexible PVC, Lead Free Gas pipe according to DIN 4815 |
|||
Density | 1.10 - 1.30 g/cc | 0.0397 - 0.0470 lb/in³ | Uncured, Part A |
3M Scotch-Weld™ EC-2815 B/A FR Epoxy Adhesive 3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a two-component epoxy adhesive with cure at room temperature or with additional heat to form a tough, impact-resistant bond. It has excellent adhesion.. |
|||
Density | 1.26 - 1.30 g/cc | 0.0455 - 0.0470 lb/in³ | ISO R 1183 |
Fainplast Compounds PHS 80/B Flexible PVC, Transparent Extrusion Pipes low migration |
|||
Density | 1.26 - 1.30 g/cc | 0.0455 - 0.0470 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 7516 Flexible PVC, Lead Free Various profiles stabilized Ca-Zn |
|||
Density | 1.26 - 1.30 g/cc | 0.0455 - 0.0470 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 0133/R Flexible PVC, Sheathing General purposes |