Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.70 g/cc | 0.278 lb/in³ | |
Piezo Kinetics 804 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type III, it is specifically used as a driver that exhibits low losses under extreme driving conditions and has a high Q. PKI 804 is well suited for medical applications.Elastic Comp.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Industeel VIRGO 39 16% Cr, 5% Ni, Martensitic Stainless Steel Description: Virgo 39 is a 16% Cr, 5% Ni, 1% Mo low carbon martensitic stainless steel. The grade is specially designed to combine high mechanical properties including toughness and improved corrosi.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
CeramTec Sonox® P6 Piezoceramic Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics .. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Williams Advanced Alloys WS205 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | As Annealed |
Eagle Brass 430 Ferritic Stainless Steel, 1/2 Hardened Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | As Annealed |
Eagle Brass 430 Ferritic Stainless Steel, 1/4 Hardened Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Crucible Steel CPM® 4V® Tool Steel CPM 4V is a powder metal tool steel with an outstanding combination of properties including high impact toughness and very good wear resistance. CPM 4V should be considered for service in fine blank.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Chicago Extruded Metals BioBrass® UNS C64200 Aluminum Bronze Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Ext.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Bohler-Uddeholm UDDEHOLM Vancron 40 nitrided powder tool steel Description: Uddeholm Vancron 40 is a nitrided powder tool steel, which means that a “surface coating” is already integrated into the finished tooling material. The result is a tool surface with v.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | Typical |
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition C AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | Typical |
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition CH 900 AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
AK Steel 409Ni Ferritic Stainless steel AK Steel 409Ni is a nominal 11% chromium stainless steel micro-alloyed with titanium, manganese and nickel that provides excellent weldability, toughness and fabricating characteristics. AK Steel 4.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Carpenter Chrome Core® 18-FM Solenoid Quality Stainless Steel, Annealed Data provided by Carpenter Technology Corporation.This is a soft ferritic material designed for operation in more corrosive environments than tolerated by 18% Cr-Fe Type 430 stainless. This new mat.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
AK Steel DI-MAX® M-36 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | Typical |
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition C AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
ATI Allegheny Ludlum 430 Ferritic Stainless Steel Characteristics:oxidation resistant at elevated temperatures, corrosion resistance approaching nickel-bearing stainless steels in mildly corrosive environments, ductile, does not work harden readily.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
ATI Allvac® Vasco® 410/403 Specialty Steel, Heat Treatment: 927°C (1700°F) Anneal Data provided by Allvac.Applications: Compressor blades, turbine parts. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 10% cold work (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 70% cold work (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Schmolz + Bickenbach Cryodur® 2379 (D-2) Cold Work Die Steel Description: Cryodur® 2379 is a high carbon, high chromium tool steel developed for high wear applications and Supplied in the annealed conditionCharacteristics: Excellent abrasive wear resistance;.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Latrobe LSS™ PGK Knife and Die Steel TLS PGK knife and die steel is a versatile medium-chromium, air-hardening tool steel that is characterized by a very good combination of toughness and wear resistance. It is available primarily in f.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
PSM Industries PolyAlloys MIM-Fe-50%Ni Grade 2 Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Density | 7.70 g/cc | 0.278 lb/in³ | |
Industeel URANUS® S1 4 % Si, Austenitic Stainless Steel Resistant to Nitric Acid Solutions Description: Research carried out in about the last fifteen years in CREUSOT LOIRE INDUSTRIE laboratories shows that a strong addition of silicon to austenitic stainless steels of the 18/10 type has.. |
|||
Density | 7.70 g/cc @Temperature 399 °C |
0.278 lb/in³ @Temperature 750 °F |
hardened to 62 HRC |
Bohler-Uddeholm O1 Cold Work Tool Steel Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface ha.. |