Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bohler-Uddeholm UDDEHOLM Vancron 40 nitrided powder tool steel

Category Metal , Ferrous Metal , Tool Steel , Cold Work Steel
Manufacturer Bohler-Uddeholm
Trade Name UDDEHOLM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bohler-Uddeholm UDDEHOLM Vancron 40 nitrided powder tool steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Uddeholm Vancron 40 is a nitrided powder tool steel, which means that a “surface coating” is already integrated into the finished tooling material. The result is a tool surface with very low friction that reduces galling or sticking of the material. Uddeholm Vancron 40 offers the possibility of eliminating time- and cost-consuming surface coatings like CVD, PVD or TD. This is achieved already in the manufacturing process of Uddeholm Vancron 40 by introducing an extra nitriding operation.Uddeholm Vancron 40 is characterized by:Very high adhesive wear resistanceVery high galling resistanceGood chipping and cracking resistanceHigh compressive strengthGood through hardening propertiesGood dimensional stability in hardeningVery good resistance to tempering backGood WEDM properties Applications: Uddeholm Vancron 40 is a cold work tool steel with an excellent galling/adhesive wear profile, which makes the steel ideal for severe production conditions and/or long run production in applications where surface coated tool steel is needed. The work materials in these applications are often soft/adherent materials such as austenitic and ferritic stainless steel, mild steel, copper, aluminium, etc. Uddeholm Vancron 40 should be used in cold work applications where the predominant failure mechanisms are adhesive wear or galling. Typical applications are: Blanking and forming; Cold extrusion; Deep drawing; and Powder pressing.
Physical Properties Metric English Comments
Density 7.70 g/cc
0.278 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 300
300
Soft annealed
Hardness, Rockwell C 61
61
Modulus of Elasticity 213 GPa

@Temperature 400 °C
30900 ksi

@Temperature 752 °F
227.0 GPa

@Temperature 200 °C
32920 ksi

@Temperature 392 °F
236 GPa

@Temperature 20.0 °C
34200 ksi

@Temperature 68.0 °F
Compressive Strength 2200 MPa
319000 psi
Rc0.2; at HRC=58
2500 MPa
363000 psi
Rc0.2; at HRC=60
2700 MPa
392000 psi
Rc0.2; at HRC=62
3000 MPa
435000 psi
Rc0.2; at HRC=64
Thermal Properties Metric English Comments
CTE, linear 11.1 µm/m-°C

@Temperature 20.0 - 200 °C
6.17 µin/in-°F

@Temperature 68.0 - 392 °F
11.9 µm/m-°C

@Temperature 20.0 - 400 °C
6.61 µin/in-°F

@Temperature 68.0 - 752 °F
Specific Heat Capacity 0.460 J/g-°C
0.110 BTU/lb-°F
Thermal Conductivity 19.0 - 23.0 W/m-K

@Temperature 200 °C
132 - 160 BTU-in/hr-ft²-°F

@Temperature 392 °F
24.5 - 25.5 W/m-K

@Temperature 400 °C
170 - 177 BTU-in/hr-ft²-°F

@Temperature 752 °F
Component Elements Properties Metric English Comments
Carbon, C 1.1 %
1.1 %
Chromium, Cr 4.5 %
4.5 %
Iron, Fe 76.3 %
76.3 %
As Balance
Manganese, Mn 0.40 %
0.40 %
Molybdenum, Mo 3.2 %
3.2 %
Nitrogen, N 1.8 %
1.8 %
Silicon, Si 0.50 %
0.50 %
Tungsten, W 3.7 %
3.7 %
Vanadium, V 8.5 %
8.5 %
Users viewing this material also viewed the following: