Material Notes:
CPM 4V is a powder metal tool steel with an outstanding combination of properties including high impact toughness and very good wear resistance. CPM 4V should be considered for service in fine blanking, powder compaction tools, for processing high-strength low-alloy (HSLA) steels, advanced high-strength steels (AHSS) and applications where a combination of strength , wear resistance and toughness is required. CPM 4V should be considered for applications where a higher attainable hardness and additional abrasion resistance is required than can be offered by CPM 3V.Information provided by Crucible Industries
Physical Properties Metric English Comments
Density 7.70 g/cc
0.278 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C >= 44

@Tempering Temp. 621 °C
>= 44

@Tempering Temp. 1150 °F
austenitizied at 1800°F, then quenched and tempered
50

@Tempering Temp. 621 °C
50

@Tempering Temp. 1150 °F
austenitizied at 1950°F, then quenched and tempered
55

@Tempering Temp. 593 °C
55

@Tempering Temp. 1100 °F
austenitizied at 1950°F, then quenched and tempered
60

@Tempering Temp. 566 °C
60

@Tempering Temp. 1050 °F
austenitizied at 1950°F, then quenched and tempered
62

@Tempering Temp. 538 °C
62

@Tempering Temp. 1000 °F
austenitizied at 1950°F, then quenched and tempered
<= 64

@Tempering Temp. 538 °C
<= 64

@Tempering Temp. 1000 °F
austenitizied at 2100°F, then quenched and tempered
Modulus of Elasticity 207 GPa
30000 ksi
Charpy Impact 48.8 J

@Treatment Temp. 1120 °C
36.0 ft-lb

@Treatment Temp. 2050 °F
austenitized; C-notch
67.8 J

@Treatment Temp. 1070 °C
50.0 ft-lb

@Treatment Temp. 1950 °F
austenitized; C-notch
74.6 J

@Treatment Temp. 982 °C
55.0 ft-lb

@Treatment Temp. 1800 °F
austenitized; C-notch
Thermal Properties Metric English Comments
Specific Heat Capacity 0.460 J/g-°C
0.110 BTU/lb-°F
Component Elements Properties Metric English Comments
Carbon, C 1.35 %
1.35 %
Chromium, Cr 5.0 %
5.0 %
Iron, Fe 85.65 %
85.65 %
as balance
Manganese, Mn 0.40 %
0.40 %
Molybdenum, Mo 2.95 %
2.95 %
Silicon, Si 0.80 %
0.80 %
Vanadium, V 3.85 %
3.85 %