Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco ASPECT® 3000 Wollastonite High aspect ratio grade. It is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. .. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco HARRP™ 20 X 40 Wollastonite HARRP™ 20X40 is suggested for concrete and concrete roof tile reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco M1250 AS WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco M1250 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco M3 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco M325 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco M400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco MD400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco MG WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco NYAD® 1250 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco NYAD® 325 Wollastonite Powdered grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particl.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco NYAD® 5000 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco NYAD® M100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco NYAD® M325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco NYCOR® R Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco NYGLOS® 12 Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco NYGLOS® 4W Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco NYGLOS® 8 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco NYGLOS® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco NYGLOS® M50 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco RRIMGLOS® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
NanoScale NanoActive® Aluminum Oxide Plus NanoActive Al2O3 Plus is produced using proprietary processes to obtain high specific surface area, high porosity (75% are mesopores), low density, weakly aggregated material possessing high adsorpt.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Ferro IP 900 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Si-Pb-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | ASTM D792 |
Techmer ES Plastiblend® PA6 SF80 L Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite (80%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Loctite® 3882 Flexible Isotropic Epoxy Adhesive Electrically Conductive BondersLoctite® Electrically Conductive Adhesives are used in a variety of applications where electrical connectivity is needed, providing a conductive path where traditiona.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | ASTM D1475 |
Aptek 6500-PMF Electrically conductive epoxy adhesive High purity, low outgassing, electrically conductive adhesiveAPTEK 6500-PMF is a one component, pre-mixed frozen, 100% solid, silver-filled epoxy adhesive specifically designed for microelectronic d.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco ULTRAFIBRE® 30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco ULTRAFIBRE® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Density | 2.90 g/cc | 0.105 lb/in³ | |
Nyco ULTRAFIBRE® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |