Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting dem.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Mykroy/Mycalex MM 451 Molding Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwid.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series A-100 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series A-205 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0040 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0070 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0100 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0230 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0337 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series Premium 4MM Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series Glass Spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0120 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series Premium 3MM Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries Ballotini® Impact Beads Ballotini® impact beads are microspheres are used for precise metal finishing of parts. They offer an environmentally safe and cost effective method for metal surface cleaning and finishing. Coars.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
GBC 496 Alumino Silicate Ceramic Propriety composition with CTE equivalent to Pyrex® glass. Can seal directly to 7070 glass, Pyrex®, or other grades of silicon. Has excellent thermal shock resistance, low firing temperature.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
GBC L3 Steatite Ideal for high frequency, low loss, high voltage insulation. Much less expensive than alumina insulatorsApplications: resistor forms, surge arrestors, standoffs, spacers, and coil forms.Machinabili.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
MMCC Aluminum/Graphite Fiber GA 7-230 Metal Matrix Composite Discontinuous graphite fiber aluminum product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plate.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Misumi Machinable SiO2-MgO Ceramic Information provided by MISUMI Corporation. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Misumi Steatite MgO-SiO2Information provided by MISUMI Corporation. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Mo-Sci Corporation GL-0275-S Class VI Soda-Lime Spheres Appearance: Solid soda-lime glass microspheres with light green color in powder form.Typical applications of GL0275-S beads including: high temperature spacer material for gauge control, coating, fi.. |
|||
Density | 2.50 - 3.30 g/cc | 0.0903 - 0.119 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 583.054 Chromium Carbide-Nickel 83-17 (Cr3C2-Ni) |
|||
Density | 2.50 - 3.20 g/cc | 0.0903 - 0.116 lb/in³ | ASTM B417 |
H.C. Starck Amperit® 588.059 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) |
|||
Density | 2.50 g/cc @Temperature 25.0 °C |
0.0903 lb/in³ @Temperature 77.0 °F |
|
Schott ILLAX® Amber Pharmaceutical Glass Amber Glass Pharmaceutical primary packaging for oralia and solid dosageInformation provided by SCHOTT AG. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Schott N-KF9 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.50 g/cc @Temperature 25.0 °C |
0.0903 lb/in³ @Temperature 77.0 °F |
|
Schott AR-GLAS® Soda Lime Silicate Glass Soda lime silicate glass, high dielectric constant, glass to metal seal, pharmaceutical primary packaging, general technical applicationInformation provided by SCHOTT AG. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec 701 Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Thermoseal KLINGER® top-chem-2000 PTFE Gasketing Fire Tested - API6FAUniversal application use in the chemical and petrochemical industriesFDA compatibleIdeal for higher temperatures and pressuresHolds shape for thermal cyclesPermits/Certification.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Arlon AD450A Glass, PTFE and Ceramic High Dielectric Constant for Circuit Militarization & Patch Antenna ApplicationsInformation provided by Arlon Materials for Electronics (MED). |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | Apparent |
Gouda Vuurvast SiC 90 Dense Refractory Brick Description: Very good thermal shock resistance, abrasion resistance as well as very good heat conductivity makes this SiC based brick very well suited for muffles as well as for applications under .. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series A-170 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Density | 2.50 g/cc | 0.0903 lb/in³ | |
Potters Industries A-Series P-0060 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |