Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.00 g/cc | 0.0723 lb/in³ | typical |
Momentive Performance Materials HBR Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Density | 2.00 - 2.80 g/cc | 0.0723 - 0.101 lb/in³ | Apparent Density; ASTM B212 |
H.C. Starck Amperit® 110.074 Agglomerated Sintered (Mo-Mo2C) |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ISO 1183 |
Hexion UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability, very slight post shrinkage, good mechanical properties, increased electrical value.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792 |
Techmer ES HiFill® TPX-PBT-98010 BN069 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityAppearance: Light BeigeProcessing Method: Injection MoldingInformation provided by TP C.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | LE 4460; ASTM D792 |
Borealis Visico™ LE4421/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4421/LE4460/LE4437 is a natural, halogen-based, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination o.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792 |
Plastics Group Polifil® BS-70 70% Barium Sulfate Reinforced Polypropylene Polifil® BS series compounds are homopolymer polypropylene resins reinforced with barium sulfate. They possess increased specific gravity, high flex modulus, high deflection temperature, good chemi.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792 - ISO 1183 |
DuPont Keldax® 6868 Filled Thermoplastic Ethylene Polymer A low fog filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications.Processing Method: ExtrusionSheetAvailabil.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ISO 1183 |
Polyram Metal Cap PB360B60 Nylon 6, 60% Mineral Filled, Heavy Density 60% Mineral filled, heavy density Nylon 6 for injection molding metalized part and galvanized covers.Information provided by Polyram. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | |
Cosmic Plastics E4930 Mineral & Glass Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | |
Du-Co Ceramics DC-142 Aluminum Silicate Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | Filament Property. |
Cytec Thornel® Mat VMA Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Composed of high strength, high modulus carbon filaments in a random-layered orientation. The fine diameter filaments are up to th.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | Filament Property. |
Cytec Thornel® Mat VMC Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Prepared by sectioning mat VMA into cubes ~ 0.5x0.5x1.0 in. VMC can be heterogeneously dispersed in matrix materials and thus enha.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | Filament Property. |
Cytec Thornel® Mat VMD Carbon Fiber Data provided by the manufacturer, Amoco Performance Products, Inc.Form of mat VMA with shorter fibers for injection molding. Fiber lengths average 400 µm - adequate for good property improvement... |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | |
Cytec Thornel® P-55S 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, high modulus strands made from a pitch precursor. The fiber surface has been treated to increase the interla.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | |
Cytec Thornel® P-75S 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus strands made from a pitch precursor. The fiber surface has been treated to increase the i.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ISO 1183/A |
Addiplast Addilene J 522 K20 Polypropylene Copolymer High densityInformation provided by Addiplast. |
|||
Density | 2.00 - 2.05 g/cc | 0.0723 - 0.0741 lb/in³ | |
Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled |
|||
Density | 2.00 - 2.15 g/cc | 0.0723 - 0.0777 lb/in³ | |
Aremco Ceramabond™ 835-MB High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792A |
Resinoid 1320 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792A |
Resinoid 1322 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792A |
Resinoid 1323 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792A |
Resinoid 1324 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | |
Cosmic Plastics CP7312 Epoxy Molding Compound Data provided by the manufacturer. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® BR111 is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical .. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | ASTM D792 |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 50 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Density | 2.00 g/cc | 0.0723 lb/in³ | |
Cosmic Plastics 3D36 Thermoset Polyester Molding Compound Data provided by the manufacturer. |