Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792-91 |
Multibase Multi-Flex® TPO D 6713 Data provided by Multibase. |
|||
Density | 1.17 - 1.18 g/cc | 0.0423 - 0.0426 lb/in³ | Polymerized; ASTM D792 |
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
SABIC Innovative Plastics GELOY HRA222 ASA GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. Use for exterior/interior electrical applications requiring UV resistance. |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
Polykemi AB SCANAMID 66 A43^E F14 Nylon 66, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
Polykemi AB SCANMID 6 B12^ NH11L Nylon 6, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
Kuraray Genestarâ„¢ N1002A-M41 Nylon Low friction unreinforced injection grade. Main Features:Low friction coefficientLow wearExamples of applications are:Friction and wear applicationGear and wheel |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
Lavergne VYTEEN PC/ABS 8515 Polycarbonate - Acrylonitrile Butadiene Styrene Alloy Vyteen PC/ABS 8515 is an enhanced PC/ABS alloy with balanced impact/stiffness properties designed for injection molding applications.Features: -High resilience -Excellent processability -High def.. |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA 6/10 (Asia Pacific) LNP* Lubricomp* QAP22S is a compound based on Nylon 6/10 resin containing PTFE, Aramid Fiber, Silicone. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 LNP* LUBRICOMP* RN001S is a compound based on Nylon 66 resin containing 2% MOS2. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRILOY D2000AXH PC LNP LUBRILOY* D2000AXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF10 L 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Asia Pacific) PC+Polyester, UV Stabilized, Transparent |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP AX08306 ABS LNP* THERMOCOMP* AX08306 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable. |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
Techmer ES Plastiblend® PC/PBT IM 6120 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA4/6 GF5 IM HS BK 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact Modifie.. |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
Borealis LE0310-99 Polyethylene Thermoplastic Semiconductive Compound LE0310-99 has the same melt flow properties as the peroxide containing material. Application: LE0310-99 is used during start up of a triple-head line. It helps to use a non-peroxide-containing mate.. |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | |
Trelleborg Emerson & Cuming Eccobond® 24 Two-Component High Strength-Impact Resistant Epoxy Adhesive Emerson & Cuming 24 Eccobond® Two-Component High Strength-Impact Resistant Epoxy AdhesiveClear, low viscosity, room temperature curing, epoxy adhesive. Exhibits resilient bonds when joining dissimi.. |
|||
Density | 1.17 g/cc @Temperature 23.0 °C |
0.0423 lb/in³ @Temperature 73.4 °F |
ASTM D1928 |
Trelleborg Horda Cable E8560 Strippable Semiconductive Shielding E8560 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8560 meets the requirements as bel.. |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
Eastman Tenite Propionate 307A2R30013 Natural, Trsp Cellulose Acetate Propionate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® K225-KWS Nylon 6 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 58 Flexible PVC, Injection Molding for Footwear Antislip soles |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 63 Medical Flexible PVC, Extrusion Tubolar apparatus |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds PG 60 Flexible PVC, Extrusion Modified with Rubber Gaskets modified with rubber |
|||
Density | 1.17 g/cc | 0.0424 lb/in³ | Part A |
Abatron AboCast 8103-23 High-Performance Dielectric Epoxy AboCast 8103-23 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has a comb.. |
|||
Density | 1.17 g/cc | 0.0423 lb/in³ | A Component; ASTM D1475 |
Aptek 6513-A/B Versatile, fast set adhesive APTEK 6513-A/B is a hazy clear, two component, general purpose, semi-rigid, paste adhesive for bonding to steel, aluminum, wood, concrete, glass, ceramics, bras, and a variety of plastics. It is sp.. |
|||
Density | 1.17 - 1.87 g/cc | 0.0423 - 0.0676 lb/in³ | Average value: 1.51 g/cc Grade Count:105 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |