Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.995 g/cc | 0.0359 lb/in³ | ISO 1183-1 |
Quadrant EPP TIVAR® MD PE-UHMW + metal detectable additive (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains a metal detectable additive which does hardly affect the inherent PE-UHMW key properties. TIVAR MD presents excellent toughne.. |
|||
Density | 0.995 g/cc | 0.0359 lb/in³ | Melt |
Covestro Apec® 1700 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay.. |
|||
Density | 0.995 g/cc | 0.0359 lb/in³ | Melt |
Covestro Apec® DP 1-9349/5 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Density | 0.995 g/cc | 0.0359 lb/in³ | Melt |
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (Conditioned) Key Features:Contains FillerSuitable processing methods:Injection molding |
|||
Density | 0.995 g/cc | 0.0359 lb/in³ | Melt |
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (DAM) Key Features:Contains FillerSuitable processing methods:Injection molding |
|||
Density | 0.995 - 1.05 g/cc | 0.0359 - 0.0381 lb/in³ | |
Lord Adhesives 506 Semi-Flexible, Medium Cure, Medium Viscosity Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Density | 0.995 - 1.05 g/cc | 0.0359 - 0.0381 lb/in³ | |
Lord Adhesives 510 Fast Cure Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Density | 0.995 - 1.02 g/cc | 0.0359 - 0.0368 lb/in³ | |
Lord Adhesives 513 Fast Cure, Non-Sagging Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Density | 0.995 g/cc | 0.0359 lb/in³ | |
Solvay CATAFOR® PU Surfactant Identification: QUATERNARY AMMONIUM ETHOSULPHATECAS: 68308 – 64 – 5Solubility: Readily soluble in water and many organic solvents.Solvent: 1-4 butanediol 20%Available in: Asia Pacific, Eu.. |
|||
Density | 0.995 g/cc | 0.0359 lb/in³ | ISO 1183 |
SYNTHOS Krasten® FB28 High Impact Polystyrene And Polyethylene Blend Polymer blend HIPS/PE. High toughness, very good tensile properties and environmental stress cracking resistance. Processed mainly by extrusion and thermoforming. Production of sheets and films, tec.. |
|||
Density | 0.995 g/cc @Temperature 330 °C |
0.0359 lb/in³ @Temperature 626 °F |
Melt |
Covestro Apec® 1703 Polycarbonate UV-stabilizedsoftening temperature (VST/B 120)=171 °CPreprocessingMax. Water content |
|||
Density | 0.995 g/cc @Temperature 330 °C |
0.0359 lb/in³ @Temperature 626 °F |
Melt |
Covestro Apec® 1745 Polycarbonate Easy to demoldsuitable for superheated steam sterilization up to 143 °C as well as for pharmaceutical applications according to United States Pharmacopeia (USP) XXII Class VIsoftening temperature (.. |
|||
Density | 0.995 g/cc @Temperature 330 °C |
0.0359 lb/in³ @Temperature 626 °F |
Melt |
Covestro Apec® 1795 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=173°CPreprocessingMax. Water content |
|||
Density | 0.995 g/cc @Temperature 240 °C |
0.0359 lb/in³ @Temperature 464 °F |
Melt |
Covestro Bayblend® FR 3002 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradefor notebooks and thinwall applicationsVicat/B 120 temperature = 99 °CUL-listing 94 V-0 (1.2 mm)antimony- chlorine- and bromine-free flame retardantglow wire test (GWFI): 960.. |
|||
Density | 0.995 g/cc | 0.0359 lb/in³ | |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |
|||
Density | 0.995 g/cc @Temperature 15.0 °C |
0.0359 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Solvesso™ 200 ND Aromatic Fluid Appearance: Transparent - Slight Yellow LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil |
|||
Density | 0.995 g/cc | 0.0359 lb/in³ | ISO 1183 |
Total ESD 201 B HDPE blow molding FINATHENE® ESD 201 B is a black conductive compound manufactured from high performance Finathene high density polyethylene. The use of this HDPE compound gives outstanding compatibility to (semi) h.. |