Polymer Property : Density = 0.956 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ASTM D1505
SABIC M200056 High Density Polyethylene for Injection Molding
Product Description: M200056 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good flow..
Density 0.956 g/cc
0.0345 lb/in³
ASTM D792
NOVA Chemicals Novapol® HB-Y556-A HDPE Extrusion Resin  (discontinued **)
Molded Plaque Properties. Features: Excellent ESCR, high rigidity and impact strength, good melt strength.Applications: chemical bottles, toys, blend for use with post-consumer resins.Data provided..
Density 0.956 g/cc
0.0345 lb/in³
ASTM D792
NOVA Chemicals Novapol® HE-Y356-A HDPE Extrusion Resin  (discontinued **)
Features: easy processing.Applications: corrugated tubing, profile extrusions, sheet extrusion and thermoforming.Data provided by the manufacturer.
Density 0.956 g/cc
0.0345 lb/in³
ASTM D1505
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade  (discontinued **)
ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo..
Density 0.956 g/cc
0.0345 lb/in³
ASTM D1505
Reliance Industries Relene F56003 Polyethylene
Relene F56003 is a High Density Polyethylene grade suitable for producing blown parts with excellent drawdown and paper like feel. It is recommended for making carrier bags and coextruded film stru..
Density 0.956 g/cc
0.0345 lb/in³
ASTM D792
Global BM-3245-PC High Density Polyethylene, Pipe Extrusion Grade
Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- ropes, fishing net, wire & cable insulators, auto parts, pipesMeets FDA requirements as listed..
Density 0.956 g/cc
0.0345 lb/in³
ASTM D1505
Global F-7000 High Density Polyethylene
Description-high quality is suitable for blown film @wide range of size & thickness Applications-large & small rolled film, shopping bag, merchant bag, disposal waste bagInformation provided by Glob..
Density 0.956 g/cc
0.0345 lb/in³
ASTM D4883
Ineos K44-08-123 HDPE Copolymer with Carbon Black
Fortiflex® K44-08-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized..
Density 0.956 - 0.962 g/cc
0.0345 - 0.0348 lb/in³
ASTM D792-98
Ipiranga Petrochem HC 7260 HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Density 0.956 - 0.962 g/cc
0.0345 - 0.0348 lb/in³
ASTM D792-98
Ipiranga Petrochem HC 7260 LS-L HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Density 0.956 g/cc
0.0345 lb/in³
ISO 1183
Iran Petrochemical (PCC) EX 4 HM9455 F High Density Polyethylene
EX4 is a high density polyethylene with 1-Butene as co monomer. It is high rigidity, low gel level, high drowdown, somewhat stiffer than EX 5.Applications: film extrusion, blending partner, refuse ..
Density 0.956 g/cc
0.0345 lb/in³
ASTM D792
IRPC Polimaxx Polene AM3245 PC High Density Polyethylene
CHARACTERISTICS:GOOD EXTRUDABILITYHIGH PRESSURE PIPE FOLLOW-UP MINIMUM REQUIRED STRENGTH OF 10.0 MPa (DESIGN STRESS OF 8.0 MPa) CLASSIFICATION PE100BLACK COLOR COMPOUNDAPPLICATIONS: PIPE EXTRUSIONSU..
Density 0.956 g/cc
0.0345 lb/in³
JPJ Technologies 1600J HDPE Extrusion
Information provided by JPJ Technologies
Density 0.956 g/cc
0.0345 lb/in³
JPJ Technologies 7800M HDPE Extrusion
Information provided by JPJ Technologies
Density >= 0.956 g/cc
>= 0.0345 lb/in³
ASTM D1505
LyondellBasell Alathon® L5876 High Density Polyethylene, Blow Molding Grade
ALATHON L5876 is designed for injection blow molding and extrusion blow molding applications where higher gloss than standard grades is required. Regulatory Status: L5876 meets the requirements of t..
Density 0.956 g/cc
0.0345 lb/in³
ISO 1183
Iran Petrochemical (PCC) EX 2 HF 7750 High Density Polyethylene
EX2 (HF 7750) is high density polyethylene with propylene as co monomer. It has a medium molar mass with a narrow molar mass distribution.Application: production of monofilaments with high tensile..
Density 0.956 g/cc
0.0345 lb/in³
Base Resin; ISO 1183
Borealis BorPEX™ HE2550 High Density Polyethylene Powder for Crosslinked Pipes
BorPEX HE2550 is a high molecular weight, high density polyethylene powder for crosslinkable pipes, specially designed for peroxide crosslinking. It is a special polymer, stabilized for transportin..
Density 0.956 g/cc
0.0345 lb/in³
Base Resin; ISO 1183
Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide))
BorPEX HE2557 is a yellow, high molecular weight, high density polyethylene compound for crosslinkable pipes, specially designed for peroxide crosslinking. Long term stability and UV resistance is ..
Density 0.956 g/cc
0.0345 lb/in³
ISO 1183
Borealis Borstar® HE3410 HDPE for Sewage Pipes
Borstar® HE3410 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an ..
Density 0.956 g/cc
0.0345 lb/in³
Compound; ISO 1183
Borealis Borstar® HE3470-LS Black HDPE Compound for Pressure Pipes
Borstar HE3470-LS is a black, high density polyethylene compound classified as an MRS 8.0 material (PE80) produced by the advanced Borstar technology. Well dispersed carbon black gives outstanding ..
Density 0.956 g/cc
0.0345 lb/in³
ISO 1183
Borealis FS1560 High Density Polyethylene
FS1560 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1560 have high impact and tensile strength, and bala..
Density 0.956 g/cc
0.0345 lb/in³
ISO 1183
Unipetrol PE HD LITEN® LS 87 HDPE
Made for special applicationsInformation provided by Unipetrol RPA
Density 0.956 g/cc
0.0345 lb/in³
ExxonMobil method
ExxonMobil Escorene™ UL 04533EH2 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 04533EH2 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Fre..
Density 0.956 g/cc
0.0345 lb/in³
ASTM D4883
ExxonMobil HDPE HD 9830.02 High Density Polyethylene Resin
Product Description: HD 9830.02 is a blow molding grade high density polyethylene copolymer with a bimodal molecular weight distribution. It provides a very good balance of stress crack resistance, ..
Density 0.956 g/cc
0.0345 lb/in³
ASTM D4883
ExxonMobil HDPE HMA 016 High Density Polyethylene Resin
Product Description: HMA 016 is a HDPE grade, characterized by fast cycling and good impact strength. It has high gloss and high dimensional stability.Availability: Africa & Middle East, Asia Pacifi..
Density 0.956 g/cc
0.0345 lb/in³
ASTM D792
Entec Hypel® PEHD18/.956 HDPE
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Density 0.956 g/cc
0.0345 lb/in³
ASTM-D792
Braskem GF4950 HDPE Blow Molding Polyethylene Copolymer
HDPE GF4950 is a high-density polyethylene copolymer with well balanced properties between impact and stiffness combined with high environmental stress cracking resistance and processability. It was..
Density 0.956 g/cc
0.0345 lb/in³
BASF DODA 4,9-Dioxadodecane,1-12-diamine
Formula: C
Density 0.956 g/cc
0.0345 lb/in³
Exxon Method
ExxonMobil Iotek® 8020 Sodium Ionomer Molding/Extrusion Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature ..
Density 0.956 g/cc
0.0345 lb/in³
Exxon Method
ExxonMobil Iotek® 8030 Sodium Ionomer Molding/Extrusion Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.Excellent abrasion resistance, impact strength, hardness, and tensile strength. Iotek ionomers provide superb low temperature impact strength when ..