Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
ASTM D1505
Polimeros Mexicanos Rotolene® ECO-BLACK Linear Medium Density Polyethylene
MDPE Copolymer with UV8 stabilizer, available as black powder.Recommended for rotomolding. Used for manufacture of septic tanks and garbage bins. Recommended for use in combination with ROTOFOAM B..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D4883
ExxonMobil LLP8455.24 Rotational Molding Resin  (discontinued **)
LL 8450 is a linear low density butene copolymer designed to offer excellent processability, whiteness and fast grinding rate. This resin is ideally suited for applications that require excellent di..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D1505
Formosa Plastics Formolene® L63565 Rotational Molding LLDPE  (discontinued **)
Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Meets all requirements of the U.S. Food and Drug Administration as spec..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D1505
Formosa Plastics Formolene® L63565U Rotational Molding LLDPE  (discontinued **)
Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Formolene L63565U is fully heat and UV stabilized.Meets all requirement..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D792
DuPont Bynel® E403 Acid-Modified Ethylene Terpolymer Adhesive Resin  (discontinued **)
Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature ..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D792
NOVA Chemicals Sclair® 14K3 Octene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer.
Density 0.936 g/cc
0.0338 lb/in³
ASTM D792
NOVA Chemicals Sclair® 8406 UV8D, 8406G UV8D MDPE Rotational Molding Resin  (discontinued **)
Features: Good balance of properties between SCLAIR® 8307 and 8405.Applications: General purpose.Data provided by the manufacturer.
Density 0.936 g/cc
0.0338 lb/in³
ASTM D792
NOVA Chemicals Sclair® 14L1 Octene LMDPE Film Resin  (discontinued **)
Low gel, Good clarity, Excellent sealing characteristicsApplications: Lamination, Co-extrusionAdditives: Process stabilizer, polymer process aidFilm properties are typical of blown film extruded at ..
Density 0.936 g/cc
0.0338 lb/in³
LyondellBasell Lupolen® 2012 D SW 413 LDPE
Cable sheathingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Density 0.936 g/cc
0.0338 lb/in³
ASTM D1505
ICO Polymers ICORENEâ„¢ 195-1325 LMDPE Rotational Molding Resin
Description: ICORENE 195-1325 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Ke..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D1505-98
Ipiranga Petrochem MB 0310 MDPE
IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D792-91
Micropol Microstat ML21 Linear medium density static dissipative polyethylene
Information provided by Micropol Limited
Density 0.936 g/cc
0.0338 lb/in³
Base Resin; ISO 1183
Borealis BorPEX™ ME2592 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))
BorPEXME2592 is a natural, high molecular weight, medium density polyethylene for crosslinkable pipes with excellent flexibility. The compound is especially designed for electron beam irradiation c..
Density 0.936 g/cc
0.0338 lb/in³
ExxonMobil method
ExxonMobil LLDPE LL 6301RQ Molding Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 6301 series are medium flow LLDPE grades, with a relatively molecular weight, resulting in molded articles which are very tough and exhibit excellent environmental stress cra..
Density 0.936 g/cc
0.0338 lb/in³
ExxonMobil method
ExxonMobil LLDPE LL 8555.24 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Density 0.936 g/cc
0.0338 lb/in³
ExxonMobil method
ExxonMobil LLDPE LL 8555.25 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Density 0.936 g/cc
0.0338 lb/in³
ExxonMobil method
ExxonMobil LLDPE LLP 8555.24 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Density 0.936 g/cc
0.0338 lb/in³
ExxonMobil method
ExxonMobil LLDPE LLP 8555.25 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D4883
ExxonMobil LLP8555.24 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D4883
ExxonMobil LLP8555.25 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Density 0.936 g/cc
0.0338 lb/in³
ExxonMobil Method
ExxonMobil Pax-Plus™ 3201 Blown Film Resin
Pax-Plus 3201 is a rubber modified high density polyethylene film resin that exhibits excellent impact strength and stress crack resistance. It is used primarily in film where its good tear resista..
Density 0.936 g/cc
0.0338 lb/in³
ExxonMobil Method
ExxonMobil Pax-Plus™ 3208 Blown Film Resin
Pax-Plus 3208 is a rubber modified high density polyethylene film resin offering good physical properties with ease of processing. It exhibits toughness, stress crack resistance and low WVTR.Inform..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D-1505
Bapolene® 345F Medium Density Polyethylene Film Resin
Description: Bapolene 345F is a medium molecular weight film resin with excellent tensile, impact, and tear properties. Applications: Merchandise bags, produce and trash bags.Bapolene® and Bapolan®..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D4883
ExxonMobil LL 8555.67 Rotational Molding Resin  (discontinued **)
LL 8555 is a linear low density hexene copolymer designed to offer excellent processability, dimensional control, whiteness and low warpage. This resin is ideally suited for applications that requir..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D1505
Huntsman Rexell® M3105 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low medium density copolymer, cast film extrusion, FDA compliantFeatures: Excellent combination of toughness, stiffness, and water vapor barrier with good temperature resistance.Applications:..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D1505
Huntsman Rexell® M3107 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low medium density copolymer, cast film extrusion, FDA compliantFeatures: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, ..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D792
NOVA Chemicals Sclair® 14B1 Butene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer.
Density 0.936 g/cc
0.0338 lb/in³
ExxonMobil method
ExxonMobil Escorene™ FL 00112 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00112 is a copolymer of ethylene and vinyl acetate offering low gel. Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No App..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D4883
ExxonMobil LL 6407 Injection Molding Resin  (discontinued **)
LL 6100 is a narrow molecular weight butene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processability with minimal wa..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D792
DuPont Bynel® 3933 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin  (discontinued **)
Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..